Karakterisasi mikrostruktur film whey dengan penambahan konjac glucomannan

نویسندگان

چکیده

The research aims to observe the effect of konjac glucomannan and different types plasticizers on microstructure whey film. film was investigated using an experimental method. conducted in descriptive methods with two treatments.The treatment used concentration (P4= 2.5 %; P7= 3 %) (C1= glycerol 30 polyethylene glycol %). results showed that combination had addition concentration, % glycerol, PEG gave microstructural characteristics good surface. this determined during heating, drying process contribution gel from structure. A more homogeneous edible obtained a KGM use plasticizer where distribution mixed into protein matrix evenly (homogeneous).

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

A simple and feasible approach to purify konjac glucomannan from konjac flour--temperature effect.

A simple one-step purification process was provided to extract KGM from KF by phase separation. The results showed that appropriate temperature control was a key factor and the products were inodorous, colourless and of high purity at the optimal temperature 68 °C. In this purification, soluble sugar and starch of extracted KGM were nearly clearly reduced and up to 95%, 80% (T68) of protein and...

متن کامل

Oxidized Konjac Glucomannan as a Paper Strength Agent

A paper strength agent is an important type of chemical additive used in the papermaking industry. In this work some new paper strengthening agent samples were obtained by treating konjac glucomannan with hydrogen peroxide under acidic conditions, and their effects on paper properties were studied. Results showed that oxidized konjac glucomannan (OKG) can improve the paper properties effectivel...

متن کامل

Preparation, composition analysis and antioxidant activities of konjac oligo-glucomannan.

Konjac oligo-glucomannan (KOG) was prepared by degradation of konjac glucomannan (KG) using β-mannanase. The hydrolysis process was monitored by the viscosity of the enzymatic hydrolysates. Factors affecting the enzymatic hydrolysis of KG were investigated, and the optimum hydrolysis conditions were as follows: time 2h; temperature 50°C; pH 6.0; and enzymatic concentration 150 U/g. Under these ...

متن کامل

A Review on Konjac Glucomannan Gels: Microstructure and Application

Konjac glucomannan (KGM) has attracted extensive attention because of its biodegradable, non-toxic, harmless, and biocompatible features. Its gelation performance is one of its most significant characteristics and enables wide applications of KGM gels in food, chemical, pharmaceutical, materials, and other fields. Herein, different preparation methods of KGM gels and their microstructures were ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Agrointek: Jurnal Teknologi Industri Pertanian

سال: 2022

ISSN: ['2527-5410', '1907-8056']

DOI: https://doi.org/10.21107/agrointek.v16i3.12303