Fabrication and inspection of C/Cf-ZrB2-ZrC-SiC and C/Cf-ZrB2-SiC composite parts resistant to ablation by pressureless sintering method

In this research, the aim is to achieve strong and ablation-resistant composite parts C / Cf-ZrB2-ZrC-SiC and C / Cf-ZrB2-SiC by non-pressure sintering method. C / Cf-ZrB2-SiC samples were prepared using synthesized ZrB2 and SiC powders between layers of resin-impregnated carbon fabric. After pressing with pressure 5 times at 1600 وC and heat treatment for 2 hours in a controlled atmosphere fur...

متن کامل

Investigation of Effective Parameters on Densification of ZrB2-SiC Based Composites Using Taguchi Method

Abstract The main goal of this study is optimization of densification of ZrB2-SiC composites reinforced with chopped Cf prepared by SPS. Taguchi method is employed as statistical design of experiment (DOE) to optimize densification parameters including SiC, Cf, MoSi2, HfB2 and ZrC content, milling time of Cf and SPS parameters such as temperature, time and pressure. Each of these factors ...

متن کامل

Comparison of Cyclic Hysteresis Behavior between Cross-Ply C/SiC and SiC/SiC Ceramic-Matrix Composites

In this paper, the comparison of cyclic hysteresis behavior between cross-ply C/SiC and SiC/SiC ceramic-matrix composites (CMCs) has been investigated. The interface slip between fibers and the matrix existed in the matrix cracking mode 3 and mode 5, in which matrix cracking and interface debonding occurred in the 0° plies are considered as the major reason for hysteresis loops of cross-ply CMC...

متن کامل

Effect of Repeated Thermal Shock on Mechanical Properties of ZrB2-SiC-BN Ceramic Composites

ZrB2-20 vol.% SiC-10 vol.% h-BN (particles) ceramic composites (ZSB) were fabricated by hot pressing under inert gas protected. ZSB samples with mean size 75 × 55 × 40 mm(3) were heated using current heating method and then cooled down to low temperature by circulating water. ZSB samples repeatedly went through thermal shock with 10-50 times under various conditions, respectively. Diverse effec...

متن کامل

Oxidation of ZrB2-SiC Composites at 1600 °C: Effect of Carbides, Borides, Silicides, and Chopped Carbon Fiber

The aim of this work is to optimize the oxidation resistance of ZrB2-SiC-based composites with different additives. Effect of nine factors including SiC, Cf, MoSi2, HfB2 and ZrC contents, milling time of Cf (M.t) and SPS parameters such as temperature, time and pressure on oxidation resistance in four levels was investigated. Taguchi design was applied to explore effective parameters for ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Defence Technology

سال: 2018

ISSN: 2214-9147

DOI: 10.1016/j.dt.2018.06.014