Isothermal Aging Behaviors of Copper–Titanium–Magnesium Supersaturated Solid-Solution Alloys
نویسندگان
چکیده
منابع مشابه
Corrosion Behavior of a Fe-25at%Sn Supersaturated Solid Solution in H3PO4 Solution
Corrosion resistance of iron can be drastically improved by addition of passivating alloying elements. A supersaturated solid solution of Fe-25at%Sn was produced by mechanical alloying of commercially pure iron and tin powders for 24 hours using a planetary ball mill. Electrochemical measurements were performed on cold compacted unsintered specimens.. XRD investigation on produced alloy showed ...
متن کاملIsothermal Aging Behavior of Beta Titanium–Manganese Alloys
Although titanium is considered to be a ubiquitous element as it has the 10th-highest Clarke number of all the elements, it is actually classified as a rare metal because the current refinement process for the metal is more environmentally damaging than the processes used to refine iron and aluminum. Furthermore, the principal alloying elements of titanium alloys are very expensive, owing to th...
متن کاملEnhanced solid solution effects on the strength of nanocrystalline alloys
Solid solution strengthening in nanocrystalline alloys is studied using sputtered Ni–W as a model system. In the composition range of 0–20 at.% W, the sputtered alloys have a nanocrystalline structure with a grain size that is independent of composition. Nanoindentation of these alloys shows that solute addition increases strength to very high levels, almost in proportion to the solute content....
متن کاملConstruction of Deformation - Mechanism Maps for Metals and Solid Solution Alloys a New Approach
A new approach has been introduced to construct deformation-mechanism maps for metals and solid solution alloys. For this purpose two computer programs named DEFOR and GRAPH have been written in BASIC to be run on IBM compatible personal computers. Using these programs, deformation - mechanism maps for a number of pure metals and a solid solution alloy (Ti-6wt% Al) have been plotted and effects...
متن کاملIsothermal and Athermal Transformation of FeNiMo Alloys
Kinetic dependence of martensitic transformation and properties changes in Fe-24%Ni5%Mo alloys with different carbon content have been obtained. Internal friction method was used for the precise investigation of structural changes after austenization, during martensitic transformation at sub zero temperature and during the postheat. The influence: (i) of frequency of oscillations, (ii) rate of ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: MATERIALS TRANSACTIONS
سال: 2020
ISSN: 1345-9678,1347-5320
DOI: 10.2320/matertrans.mt-m2020149