Investigations on tensile fractography and wear characteristics of Al7075-Al2O3-SiC Hybrid Metal Matrix Composites routed through liquid metallurgical techniques

نویسندگان

چکیده

The Al2O3-SiC reinforced Al7075 Metal Matrix Composite (MMCs) is fabricated through liquid metallurgical technique. Ceramic particulates were amalgamated into aluminium alloy to achieve improved mechanical properties and wear resistance. Al-7075/Al2O3/SiC hybrid MMCs produced by reinforcing 2%, 3%, 4% 5% of Al2O3 7% SiC particles. Microstructural analysis was carried out evaluate the uniform dispersal within base matrix. output results indicate that enhanced increase wt. % ceramic particulates. Tensile fractography show internal fracture structure tensile test specimens in which pullouts observed. characteristics developed composites are studied using pin on disc apparatus. high resistance observed at + MMCs.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Studying on the fatigue behavior of Al- Al2O3 metal matrix nano composites processed through powder metallurgy

Excellent mechanical properties and fatigue performance of Al/Al2O3 metal-based nanocomposites caused to introduce this material as a good candidate for various applications. In this regard, the preparation and characterization of this composite can be considered as a hot issue for research. The study was carried out in several steps including: (i) preparation of Al/Al2O3 metal-based nanocompos...

متن کامل

Physio-mechanical Properties of Aluminium Metal Matrix Composites Reinforced with Al2O3 and SiC

Particulate reinforced metal matrix composites (MMCs) are potential materials for various applications due to their advantageous of physical and mechanical properties. This paper presents a study on the performance of stir cast Al2O3 SiC reinforced metal matrix composite materials. The results indicate that the composite materials exhibit improved physical and mechanical properties, such as, lo...

متن کامل

Casting of SiC Reinforced Metal Matrix Composites

Composites based on two aluminium alloys (A536 and 6061) reinforced with 10% or 20% volume fraction of SiC particles were produced by gravity casting and a novel two-step mixing method was applied successfully to improve the wettability and distribution of the particles. The SiC particles were observed to be located predominantly in the interdendrit ic regions, and a thermal lag model is propos...

متن کامل

Processing and Characterization of AA2024/Al2O3/SiC Reinforces Hybrid Composites Using Squeeze Casting Technique

The present requirement of automobile industry is seeking lightweight material that satisfices the technical and technological requirements with better mechanical and tribological characteristics.  Aluminium matrix composite ( AMC ) materials meet the requirements of the modern demands. AMCs are used in automotive applications as engine cylinders, pistons, disc and drum brakes. This paper inves...

متن کامل

Grinding of Aluminium-Based Metal Matrix Composites Reinforced with Al2O3 or SiC Particles

This paper presents results obtained from the grinding of aluminium-based metal matrix composites reinforced with either aluminium oxide (Al2O3) or silicon carbide (SiC) particles using grinding wheels made of SiC in a vitrified matrix or diamond in a resin-bonded matrix. The study used grinding speeds of 1100–2200 m min , a grinding depth of 15 m for rough grinding and 0.1–1 m for fine grindin...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Fracture and Structural Integrity

سال: 2021

ISSN: ['1971-8993']

DOI: https://doi.org/10.3221/igf-esis.56.13