Investigation on Microstructure and Tensile Fractography of RE Oxides (CeO2/Y2O3) Reinforced AZ91D Magnesium Matrix Composites

نویسندگان

چکیده

The current work aims to investigate the mechanical properties of rare oxide reinforced Mg alloy based MMCs. Magnesium matrix considered in study is AZ91D alloy, whereas earth oxides were CeO2 and Y2O3. Y2O3 particulate reinforcement percentage was varied from 1 3% steps 1% its influence on Stir casting route adopted fabricate sample for study. Microstructure analysis illustrated uniform distribution alloys. obtained results revealed enhanced such as tensile strength, yield elongation hardness MMCs due increased reinforcement. Fractography fracture surfaces demonstrated microcracks cleavage dominant pure alloy. While particle debonding, extensive plastics deformation prominent in-addition

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Tensile and fatigue behavior of AZ91D magnesium alloy

Recently magnesium alloys, owing to their low density and excellent specific strength have been attractive to designers as an advanced material for coping with energy conservation and environmental pollution regulations. Much of the recent developments of magnesium alloys and processes have been driven by the requirements of the aerospace industry, although some successful ones have found appli...

متن کامل

Aging behavior of nano-SiCp reinforced AZ61 magnesium matrix composites

Male, born in 1962, Ph.D, Professor. He obtained his Ph.D at Nanchang University. His research and teaching interests mainly focus on magnesium/aluminum alloys and investment casting process. He has published more than 200 papers by now. E-mail: [email protected] Received: 2011-01-25; Accepted: 2011-05-04 *Yan Hong *Yan Hong, Hu Xiaowu, Nie Qiao and Chen Lei (School of Mechanical-Electrical En...

متن کامل

Microstructure and mechanical behavior of metallic glass fiber-reinforced Al alloy matrix composites

Metallic glass-reinforced metal matrix composites are an emerging class of composite materials. The metallic nature and the high mechanical strength of the reinforcing phase offers unique possibilities for improving the engineering performance of composites. Understanding the structure at the amorphous/crystalline interfaces and the deformation behavior of these composites is of vital importanc...

متن کامل

Anomaly Detection and Microstructure Characterization in Fiber Reinforced Ceramic Matrix Composites

ANOMALY DETECTION AND MICROSTRUCTURE CHARACTERIZATION IN FIBER REINFORCED CERAMIC MATRIX COMPOSITES Name: Bricker, Stephen E. University of Dayton Advisor: Dr. Russell Hardie Ceramic matrix composites (CMCs) have the potential to replace current superalloys being used in hot components of jet engines. CMCs with continuous fiber reinforcement exhibit significant strength retention beyond tempera...

متن کامل

Microstructure and corrosion characteristics of laser-alloyed magnesium alloy AZ91D with Al-Si powder.

Blown-powder laser surface alloying was performed on the magnesium alloy AZ91D with Al-Si alloy powder to improve corrosion resistance. Characterization by scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS) and x-ray diffraction (XRD) analysis revealed that intermetallic compounds (IMCs) of Mg2Si, Al12Mg17 and Al3Mg2 were formed in the matrix of α-Mg and Al solid solutions...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Fracture and Structural Integrity

سال: 2022

ISSN: ['1971-8993']

DOI: https://doi.org/10.3221/igf-esis.63.10