Investigation of the tensile deformation behaviour in Ni-based superalloy inconel alloy 617 using EBSD-based finite element simulations and optical flow method

نویسندگان

چکیده

Abstract To improve component design, the fundamental understanding of fatigue behaviour gas turbine materials is essential. Since Ni-alloys exhibit pronounced elastic anisotropy, local grain orientation strongly affects stress and strain distribution in material under mechanical loadings. This work addresses characterisation anisotropic elastic–plastic deformation its consequences for crack initiation nickel-base superalloy IN617 tensile loading. Samples were loaded situ a scanning electron microscope (SEM) to correlate with structure determined by backscatter diffraction (EBSD) measurements. calculate resulting stresses strains, EBSD data used develop model finite element method (FEM) considering orientation. The results (FE) simulation compared theories E⋅m based on Schmidt factor (m) Young’s modulus (E). A mathematical image registration called “optical flow method” (OFM), which capable transformation measuring points during deformation, was applied data. strains calculated optical FE two samples. findings revealed large later area found both OFM FEM. developed FEM verified successful correlation hypotheses E·m simulated behaviour. Furthermore, impact microstructural neighbourhood emphasised. Graphical

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

buckling of viscoelastic composite plates using the finite strip method

در سال های اخیر، تقاضای استفاده از تئوری خطی ویسکوالاستیسیته بیشتر شده است. با افزایش استفاده از کامپوزیت های پیشرفته در صنایع هوایی و همچنین استفاده روزافزون از مواد پلیمری، اهمیت روش های دقیق طراحی و تحلیل چنین ساختارهایی بیشتر شده است. این مواد جدید از خودشان رفتارهای مکانیکی ارائه می دهند که با تئوری های الاستیسیته و ویسکوزیته، نمی توان آن ها را توصیف کرد. این مواد، خواص ویسکوالاستیک دارند....

Design of Broaching Tool Using Finite Element Method for Achieving the Lowest Residual Tensile Stress in Machining of Ti6Al4V Alloy

The aim of this study, is to use finite element simulation to achieve the optimal geometry of a broaching tool that creates the lowest tensile stress at the machined surface of the Ti6Al4V alloy. It plays a major role in reducing production costs and improves the surface integrity of the machined parts. The type and amount of residual stress determined by the thermal and mechanical loads transm...

متن کامل

Evaluation of Fracture Parameters by Coupling the Edge-Based Smoothed Finite Element Method and the Scaled Boundary Finite Element Method

This paper presents a technique to evaluate the fracture parameters by combining the edge based smoothed finite element method (ESFEM) and the scaled boundary finite element method (SBFEM). A semi-analytical solution is sought in the region close to the vicinity of the crack tip using the SBFEM, whilst, the ESFEM is used for the rest of the domain. As both methods satisfy the partition of unity...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Materials Science

سال: 2023

ISSN: ['1573-4803', '0022-2461']

DOI: https://doi.org/10.1007/s10853-023-08558-5