Investigation of the Morphological Evolution and Etching Kinetics of black Silicon During Ni-Assisted Chemical Etching
نویسندگان
چکیده
منابع مشابه
Unraveling the Morphological Evolution and Etching Kinetics of Porous Silicon Nanowires During Metal-Assisted Chemical Etching
Many potential applications of porous silicon nanowires (SiNWs) fabricated with metal-assisted chemical etching are highly dependent on the precise control of morphology for device optimization. However, the effects of key etching parameters, such as the amount of deposited metal catalyst, HF-oxidant molar ratio (χ), and solvent concentration, on the morphology and etching kinetics of the SiNWs...
متن کاملFabrication and Optical Characterization of Silicon Nanostructure Arrays by Laser Interference Lithography and Metal-Assisted Chemical Etching
In this paper metal-assisted chemical etching has been applied to pattern porous silicon regions and silicon nanohole arrays in submicron period simply by using positive photoresist as a mask layer. In order to define silicon nanostructures, Metal-assisted chemical etching (MaCE) was carried out with silver catalyst. Provided solution (or materiel) in combination with laser interference lithogr...
متن کاملHierarchical silicon nanostructured arrays via metal-assisted chemical etching
Department of Physics and Materials Scien Chee Avenue, Kowloon Tong, Kowloon, Hon Department of Biology and Chemistry, Cit Avenue, Kowloon Tong, Kowloon, Hong Kon Centre for Functional Photonics (CFP), Cit Avenue, Kowloon Tong, Kowloon, Hong Kon Shenzhen Research Institute, City Universit † Electronic supplementary informa 10.1039/c4ra06172a ‡ These authors contributed equally to th Cite this: ...
متن کاملMetal-assisted chemical etching in HFÕH2O2 produces porous silicon
A simple and effective method is presented for producing light-emitting porous silicon ~PSi!. A thin (d,10 nm! layer of Au, Pt, or Au/Pd is deposited on the ~100! Si surface prior to immersion in a solution of HF and H2O2 . Depending on the type of metal deposited and Si doping type and doping level, PSi with different morphologies and light-emitting properties is produced. PSi production occur...
متن کاملWet-Chemical Etching and Cleaning of Silicon
A Introduction Research and manufacturing related to silicon devices, circuits, and systems often relies on the wet-chemical etching of silicon wafers. The dissolution of silicon using liquid solutions is needed for deep etching and micromachining, shaping, and cleaning. Also, wet-chemistries are often used for defect delineation in single crystal silicon materials. In this paper, a review of t...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Physics: Conference Series
سال: 2018
ISSN: 1742-6588,1742-6596
DOI: 10.1088/1742-6596/987/1/012039