Investigation of the Kinetics of Borided AISI 420 and AISI 5140 Steels

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Mechanical Properties of Boronized AISI 316, AISI 1040, AISI 1045 and AISI 4140 Steels

In this study, some mechanical properties of borided and unborided four steels were investigated. Boronizing of steels was performed by powder pack method at 1210 K for 4 h. The hardness of borides, boride layer thickness and room temperature tensile properties were measured and it was observed that hardness and tensile properties strongly depend on chemical composition of steels. In addition, ...

متن کامل

Investigation of Adhesion and Tribological Behavior of Borided AISI 310 Stainless Steel

In the present study, the effects of the boriding process on adhesion and tribological properties of AISI 310 steel were investigated. Boriding was performed in a solid medium consisting of Ekabor-II powders at 1123 and 1323K for 2 and 6 h. The boride layer was characterized by optical microscopy, the X-ray diffraction technique and the micro-Vickers hardness tester. The X-ray diffraction analy...

متن کامل

Mechanical Characterization of Friction Welded AISI 304 Steels

There are many industries where austenitic stainless steel needs to be welded specially in power generation industries. Unfortunately the austenitic stainless welding has several fabrication and metallurgical drawbacks when welded by using conventional fusion welding methods, which can often leads to in-service failure. The most pronounced fabrication faults are hot cracks due to inadvertent us...

متن کامل

Corrosion and microstructural analysis data for AISI 316L and AISI 347H stainless steels after exposure to a supercritical water environment.

This article presents corrosion data and microstructural analysis data of austenitic stainless steels AISI 316L and AISI 347H exposed to supercritical water (25 MPa, 550 °C) with 2000 ppb of dissolved oxygen. The corrosion tests lasted a total of 1200 h but were interrupted at 600 h to allow measurements to be made. The microstructural data have been collected in the grain interior and at grain...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Afyon Kocatepe University Journal of Sciences and Engineering

سال: 2014

ISSN: 2147-5296,2149-3367

DOI: 10.5578/fmbd.7356