Internal curing by superabsorbent polymers in alkali-activated slag

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The Interfacial Transition Zone in Alkali-Activated Slag Mortars

The interfacial transition zone (ITZ) is known to strongly influence the mechanical and transport properties of mortars and concretes. This paper studies the ITZ between siliceous (quartz) aggregates and alkali-activated slag (AAS) binders in the context of mortar specimens. Backscattered electron (BSE) images generated in an environmental scanning electron microscope (ESEM) are used to identif...

متن کامل

SELF-Cured Alkali Activated Slag Concrete Mixes- An Experimental Study

Alkali Activated Slag Concrete (AASC) mixes are manufactured by activating ground granulated blast furnace slag (GGBFS) using sodium hydroxide and sodium silicate solutions. The aim of the present experimental research was to investigate the effect of increasing the dosages of sodium oxide (Na2O, in the range of 4 to 8%) and the activator modulus (Ms) (i.e. the SiO2/Na2O ratio, in the range of ...

متن کامل

Superabsorbent Polymers and Superabsorbent Polymer Composites

This article briefly describes the general aspects and cross-linking polymerization of superabsorbent polymers (SAPs) and superabsorbent polymer composites (SAPCs). Research and development of SAPs has become very active after the Northern Region Laboratory of the United States Department of Agriculture invented the first SAP, used as a soil conditioner. Based on the advancements in organic/ino...

متن کامل

Microstructural Changes Induced by CO2 Exposure in Alkali-Activated Slag/Metakaolin Pastes

The structural changes induced by accelerated carbonation in alkali-activated slag/ metakaolin (MK) cements were determined. The specimens were carbonated for 540 h in an environmental chamber with a CO2 concentration of 1.0 ± 0.2%, a temperature of 20 ± 2°C, and relative humidity of 65 ± 5%. Accelerated carbonation led to decalcification of the main binding phase of these cements, which is an ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Cement and Concrete Research

سال: 2020

ISSN: 0008-8846

DOI: 10.1016/j.cemconres.2020.106123