Influence of the filler material on the pitting corrosion in welded duplex stainless steel 2205

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The Influence of Heat-Input on Structural and Mechanical Properties of 2205 Duplex Stainless Steel

The influence of heat-input and pre-heat treatment on the structure, mechanical and corrosion behaviors of 2205 duplex stainless steel joint by means of GMAW process was the goal of this study. In this regards, the welding process was done using different heat input in the range of 0.6 to 1.4 kJ/mm and different pre-heating treatments in the range of 25 to 100 oC. The microstructural properties...

متن کامل

Corrosion Resistance and Semiconducting Properties of the Passive Films on Duplex Stainless Steel 2205

In this study, the effect of molybdate on the electrochemical behavior and semi-conductive properties of duplex stainless steel 2205 passive film at NaCl solutions was investigated. Cyclic potentiodynamic polarization, impedance spectroscopy, mott-schottky plots and scanning electron microscopy (SEM) were used to study the passive behavior. Polarization curves showed that the corrosion current ...

متن کامل

The Influence of Heat-Input on Structural and Mechanical Properties of 2205 Duplex Stainless Steel

The influence of heat-input and pre-heat treatment on the structure, mechanical and corrosion behaviors of 2205 duplex stainless steel joint by means of GMAW process was the goal of this study. In this regards, the welding process was done using different heat input in the range of 0.6 to 1.4 kJ/mm and different pre-heating treatments in the range of 25 to 100 oC. The microstructural properties...

متن کامل

Study on Static Recrystallization Process in Duplex Stainless Steel 2205

Steel 2205 is one of the most famous duplex stainless steels. The microstructure of this steel composed of ferrite and austenite in similar amount. Therefore, in order to improve mechanical properties through microstructure, thermo mechanical processes such as controlled hot rolling and forging should be applied. It is not possible to employ the usual heat treatment. It shows the importance of ...

متن کامل

Probabilistic Pitting Corrosion Risk Assessment of Welded Offshore Steel Pipelines

Steel structures continuously exposed to offshore marine environments are prone to corrosion. This can be of major economic and perhaps of environmental significance. The risk of these scenarios occurring can be assessed using good quality data, good quality corrosion and pitting models and structural reliability assessment. Recently, improved models for the prediction of longer term corrosion ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Revista de Metalurgia

سال: 2007

ISSN: 1988-4222,0034-8570

DOI: 10.3989/revmetalm.2007.v43.i4.70