Influence of Specimen Orientation on Susceptibility to Stress Corrosion Cracking in Extruded Magnesium Alloy AZ80

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Kinetics of SIMA AZ80 Magnesium Alloy

Semi-solid feedstock of AZ80 magnesium alloy modified by [trace] rare-earth Y element 10 (0, 0.2, 0.4, 0.8 wt.%) were fabricated by [strain-induced melting activation] (SIMA) in the form of 11 extrusion and partial remelting. The effect of Y addition on the microstructure evolution of [the] 12 extruded and [isothermally heat] treated alloy was observed by [using an] optical microscope (OM), 13 ...

متن کامل

Effect of Hydrogen on Corrosion and Stress Corrosion Cracking of AZ91 Alloy in Aqueous Solutions

The effect of hydrogen on the corrosion and stress corrosion cracking of the magnesium AZ91 alloy has been investigated in aqueous solutions. Hydrogen produced by corrosion in water diffuses into, and reacts with the Mg matrix to form hydride. Some of the hydrogen accumulates at hydride/Mg matrix (or secondary phase) interfaces as a consequence of slow hydride formation and the incompatibility ...

متن کامل

Mitigation of Corrosion on Magnesium Alloy by Predesigned Surface Corrosion

Rapid corrosion of magnesium alloys is undesirable in structural and biomedical applications and a general way to control corrosion is to form a surface barrier layer isolating the bulk materials from the external environment. Herein, based on the insights gained from the anticorrosion behavior of corrosion products, a special way to mitigate aqueous corrosion is described. The concept is based...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Society of Materials Science, Japan

سال: 2015

ISSN: 0514-5163,1880-7488

DOI: 10.2472/jsms.64.655