In-situ observation of hydrogen induced crack initiation in a nickel-based superalloy

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Crystal plasticity and crack initiation in a single-crystal nickel-base superalloy Modelling, evaluation and applications

In this dissertation the work done in the projects KME-410/502 will be presented. The overall objective in these projects is to evaluate and develop tools for designing against fatigue in single-crystal nickel-base superalloys in gas turbines. Experiments have been done on single-crystal nickel-base superalloy specimens in order to investigate the mechanical and fatigue behaviour of the materia...

متن کامل

Fatigue crack initiation in a notched single-crystal superalloy component

In this paper, the fatigue crack initiation in notched single-crystal test specimens of material MD2 is investigated and analysed. A critical plane approach is adopted, in which the total strain ranges on the discrete slip planes are evaluated. Furthermore, a Coffin-Manson type of expression is used to describe the number of cycles to fatigue crack initiation. This relation is determined from a...

متن کامل

Prediction of crack growth in a nickel-based superalloy under fatigue-oxidation conditions

Prediction of oxidation-assisted crack growth has been carried out for a nickel-based superalloy at elevated temperature based on finite element analyses of oxygen diffusion, coupled with viscoplastic deformation, near a fatigue crack tip. The material constitutive behaviour, implemented in the finite element code ABAQUS via a user-defined material subroutine (UMAT), was described by a unified ...

متن کامل

Evaluation of Fatigue Crack Initiation in a Notched Single-crystal Superalloy Component

The fatigue crack initiation in a notched single-crystal nickel-base superalloy component at 500°C was investigated and analysed. A critical plane approach in combination with a critical distance method has been adopted, in which the total shear strain ranges on the discrete slip planes are evaluated. Furthermore, a Coffin-Manson type of expression is used to predict the number of cycles to fat...

متن کامل

Analysis of Cracks in the Pulsed Nd:YAG Laser Welded Joint of Nickel-Based Superalloy

The weldability of GTD-111 nickel-based superalloy by pulsed Nd:YAG laser welding with an average power of 250 W was studied, and the microstructural evolution and cracking characteristics were also investigated. The solidification cracking of the fusion zone (FZ) and the intergranular liquation cracking in the heat affected zone (HAZ) were observed in the joint. Solidification cracking was cau...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Scripta Materialia

سال: 2017

ISSN: 1359-6462

DOI: 10.1016/j.scriptamat.2017.07.006