Improving Electrochemical Performance of Ni-rich Cathode Using Atomic Layer Deposition with Particle by Particle Coating Method
نویسندگان
چکیده
منابع مشابه
Influence of electroplating parameters on microstructure and amount of ceramic particle deposition in Ni-Co-CeO2-ZrO2 composite coating
Austenitic stainless steels are high performance steels that have various applications in solid oxide fuel cells and boiler tubes under high temperature operating conditions. The Cr2O3 oxide layer formed on the steel surface becomes unstable at high temperatures and reduces the oxidation resistance of the steel. Therefore, protection of these steels at high temperatures is essential. Therefore,...
متن کاملAnalytic expressions for atomic layer deposition: Coverage, throughput, and materials utilization in cross-flow, particle coating, and spatial atomic layer deposition
In this work, the authors present analytic models for atomic layer deposition (ALD) in three common experimental configurations: cross-flow, particle coating, and spatial ALD. These models, based on the plug-flow and well-mixed approximations, allow us to determine the minimum dose times and materials utilization for all three configurations. A comparison between the three models shows that thr...
متن کاملEnhancement of Electrochemical Performance of LiMn2O4 Spinel Cathode Material by Synergetic Substitution with Ni and S
Nickel and sulfur doped lithium manganese spinels with a nominal composition of LiMn2-xNixO4-ySy (0.1 ≤ x ≤ 0.5 and y = 0.01) were synthesized by a xerogel-type sol-gel method followed by subsequent calcinations at 300 and 650 °C in air. The samples were investigated in terms of physicochemical properties using X-ray powder diffraction (XRD), transmission electron microscopy (EDS-TEM), N₂ adsor...
متن کاملElectrochemical Monitoring of TiO2 Atomic Layer Deposition by Chronoamperometry and Scanning Electrochemical Microscopy
The scanning electrochemical microscope (SECM) was used to characterize the atomic layer deposition (ALD) of TiO2 on indium-doped tin oxide (ITO) substrates by studying electron transfer through pores in the thin films (1−5 nm thickness). The extent of electron transfer, and thus the porosity of the films, was evaluated by transient electrochemistry. These studies show that ALD deposition of Ti...
متن کاملThe Effect of LiFePO4 Coating on Electrochemical Performance of LiMn2O4 Cathode Material
LiMn2O4 spinel cathode materials have been successfully synthesized by solid-state reaction. Surface of these particles were modified by nanostructured LiFePO4 via sol gel dip coating method. Synthesized products were characterized by thermally analyzed by Thermogravimetric and Differential Thermal Analysis(TG/DTA), X-Ray Diffraction (XRD), Scanning Electron...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Electrochemical Science and Technology
سال: 2021
ISSN: 2093-8551,2288-9221
DOI: 10.33961/jecst.2020.01599