Improvement of Impact Strength for Copper/Aluminium Friction Welded Joint.

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The Strength of Friction Stir Welded and Friction Stir Processed Aluminium Alloys

Local strength of friction stir (FS) welds and FS processed aluminium alloys in heat treatable aluminium alloys is dominated by precipitation hardening. Strengthening due to stored dislocations is generally limited to 40MPa, and grain size strengthening is generally less than 10MPa. Local crystallographic texture can cause yield strength variation on the order of 5%. Published models for streng...

متن کامل

Experimental Investigation of Tensile Strength and Deflection Characteristics of Friction Stir Welded Aluminum AA 6351 Alloy Joint

Aluminum alloys are used in many applications in which the combination of high strength and low weight is attractive; ship building, air frame, transportation industry etc. are some areas in which the low weight can be significant value. Friction stir welding (FSW) is a new welding technique particularly well suited to aluminum alloys though this technique is also used for other materials. Fric...

متن کامل

Improving Fatigue Strength of Welded Joints by Ultrasonic Impact Treatment

Enhancement in fatigue performance of welded joints by Ultrasonic Impact Treatment (UIT) was evaluated with large-scale rolled beam and built-up specimens having yield strength of 345 to 760 MPa. Eighteen rolled-beam specimens having welded details at cover plates and transverse stiffeners and eight built-up specimens having only transverse stiffener details were fatigue tested after treating t...

متن کامل

Microstructure and Mechanical Properties of the Friction Welded Joint between X53CrMnNiN219 and X45CrSi93 Stainless Steel

Dissimilar metals friction welding of austenitic–martensitic stainless steels is commonly used in order to manufacture engine valves in the automobile industry. In this study, X53CrMnNiN219 (austenitic stainless steel) and X45CrSi93 (martensitic stainless steel) valve steel rods were welded by friction welding process. The welded joint was then heat treated at 760 0C for 60 min. Mechanical prop...

متن کامل

Investigation on Tensile Strength of Friction Stir Welded Joints in PP/EPDM/Clay Nanocomposites

Polymer-based nanocomposites due to their advantages such as corrosion resistance,adequate mechanical properties and low cost are widely used in modern technologies. The increasing application of these nanocomposites, and hence their welding seems unavoidable. In this paper, a novel hottool in friction stir welding process is used for butt welding nanocomposite plates of 5 mm thick containing p...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: TRANSACTIONS OF THE JAPAN SOCIETY OF MECHANICAL ENGINEERS Series A

سال: 1998

ISSN: 0387-5008,1884-8338

DOI: 10.1299/kikaia.64.2388