Improvement of Bond Strength in Metal-Ceramic Systems Using a Gold Intermediate Layer.

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

A Comparative Evaluation of Shear Bond Strength of Creation Ceramic Veneer to Metal and Zirconia Cores

Abstract Background and Aim: High chipping rates of the veneering porcelain of zirconia ceramic restorations have been reported in clinical studies. Thus, the shear bond strength (SBS) between the zirconia core and veneering porcelain requires investigation. Materials and Methods: In this in-vitro study, at first, using a computer-aided design/computer-aided manufacturing (CAD/CAM) machine, 1...

متن کامل

Factors affecting the shear bond strength of metal and ceramic brackets bonded to different ceramic surfaces.

The aims of this study were to evaluate the shear bond strength (SBS) of metal and ceramic brackets bonded to two different all-ceramic crowns, IPS Empress 2 and In-Ceram Alumina, to compare the SBS between hydrofluoric acid (HFA), phosphoric acid etched, and sandblasted, non-etched all-ceramic surfaces. Ninety-six all-ceramic crowns were fabricated resembling a maxillary left first premolar. T...

متن کامل

Bond strength durability of a resin composite on a reinforced ceramic using various repair systems.

OBJECTIVES This study compared the durability of repair bond strength of a resin composite to a reinforced ceramic after three repair systems. METHODS Alumina-reinforced feldspathic ceramic blocks (Vitadur-alpha) (N=30) were randomly divided into three groups according to the repair method: PR-Porcelain Repair Kit (Bisco) [etching with 9.5% hydrofluoric acid+silanization+adhesive]; CJ-CoJet R...

متن کامل

Effect of Surface Roughness Morphology on Bond Strength of Thermal Sprayed WC-10Co-4Cr Ceramic/Metal Coating

In this study, the effect of surface roughness and roughness morphology on the bond strength of WC-Co-Cr coatings has investigated. The three different surfaces morphology are use for this purpose. The first and tow samples sandblasted with alumina and silicon carbide respectively. Other sample no sandblasted before spraying process. The same WC-10Co-4Cr coating deposited on the substrates with...

متن کامل

assessment of bond strength between metal brackets and non-glazed ceramic in different surface treatment methods

objective:   the aim of this study was to evaluate the bond strength between metal brackets and non-glazed ceramic with three different surface treatment methods. materials and methods: forty-two non-glazed ceramic disks were assigned into three groups. group i and ii specimens were etched with 9.5% hydrofluoric acid. subsequently in group i, silane and adhesive were applied and in group ii, bo...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Dental Materials Journal

سال: 1998

ISSN: 1881-1361,0287-4547

DOI: 10.4012/dmj.17.163