Impression creep testing across a heat affected zone

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Evaluation of current methods for creep analysis and impression creep testing of power plant steels

Destructive testing of creep exposed components is a powerful tool for evaluation of remaining lifetime of high temperature pipe systems. The most common destructive evaluation method used today is uniaxial creep testing. Uniaxial creep tests can produce accurate creep curves but the test method has some drawbacks such as costliness and long testing times. It also demands large sample material ...

متن کامل

Heat Affected Zone in Surfacing Chromium Ledeburitic Steel

Repair welding is not used enough in the industry 1 . One of the reasons for this lies in the insufficient and unrealiable knowledge in many segments of this area. A very important part is having appropriate knowledge of metallurgical processes in heating of the base material 2-4 . Unsuitable heating deteriorates the microstructure as it reduces toughness and fracture behaviour of the weld 5 . ...

متن کامل

Numerical Simulation Of Heat Affected Zone Microstructure During Laser Surface Melting

Microstructural changes during laser welding and laser surface treatment has been regarded by many researchers. Most researches have focused on studying the effect of various process parameters on the size and microstructure of the heat affected zone. But some studies show that the initial microstructure of the base metal can also affect the heat affected zone dimensions and final microstructur...

متن کامل

Development of a new creep testing equipment to obtain long-term deformation parameters of salt rocks

Creep phenomenon in rock engineering plays a key role in development of underground spaces as they must be stable enough for a long period of time. Current research involved designing and manufacturing of a new creep testing machine. The equipment is capable to perform simultaneous light-duty creep tests on more than one cylindrical rock samples at a very low cost.To evaluate the equipment’s pe...

متن کامل

Microstructural Investigation of the Heat-affected Zone of Simulated Welded Joint of P91 Steel

T. Vuherer, University of Maribor, Faculty of Mechanical Engineering, Slovenia, M. Dunđer, University of Rijeka, Politechnika Department of Philosophy Faculty, Croatia, I. Samardžić, University of Osijek, Mechanical Engineering Faculty, Slav. Brod, Croatia, Lj. Milović, University of Belgrade, Faculty of Technology and Metallurgy, Serbia, M. Zrilić, University of Belgrade, Faculty of Technology...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Ubiquity Proceedings

سال: 2018

ISSN: 2631-5602