منابع مشابه
Microstructural Examination of Ni-ion Irradiated Fe-Ni-Cr Alloys Followed to Micro-zone Deformation
Examination of deformation microstructures induced by micro-indentation technique by means of transmission electron microscopy following an MV range metallic ion irradiation was performed in order to study the influence of irradiation-produced microstructural defects on plastic deformation behavior of materials. In this work, specimens of an Fe-Cr-Ni austenitic model ternary alloy before and af...
متن کاملOxidation – Nitridation of Ni-Cr-Al Alloys
A series of alloys containing 24-36 wt pct Cr and 13.5 – 25.0 wt pct Al was reacted with air at 1100 °C for 260 h. The products of isothermal reaction were scales of α-Al 2 O 3 plus small amounts of Cr 2 O 3 . These grew according to parabolic kinetics, interrupted by episodic weight losses caused by partial spallation. No nitridation occurred during the isothermal exposures. Reaction during th...
متن کاملTernary Ni-Fe-Co Alloys Nanowire Electrodeposition
Nanowire is a cylindrical nano-structure with nanometer dimensions. In this research, the studied nanowire was made from the magnetic triple Ni-Fe-Co alloy.
 We utilized ordered porous anodic aluminum oxide as a template for the nanowire deposition. The nanowire arrays were electrodeposited in the cylindrical pores of the oxide layer by AC potential in a simple sulfate bath. Then the relatio...
متن کاملTernary Ni-Fe-Co Alloys Nanowire Electrodeposition
Nanowire is a cylindrical nano-structure with nanometer dimensions. In this research, the studied nanowire was made from the magnetic triple Ni-Fe-Co alloy. We utilized ordered porous anodic aluminum oxide as a template for the nanowire deposition. The nanowire arrays were electrodeposited in the cylindrical pores of the oxide layer by AC potential in a simple sulfate bath. Then the relation ...
متن کاملLaser Welded Ni-Cr Dental Alloys Inspection
Minor problems arising from optimizations by welding of fixed prostheses frameworks can be identified by macroscopic and microscopic visual inspection. The purpose of this study was to highlight the visible discontinuities present in the laser welds of dental Ni-Cr alloys. Ni-Cr base metal alloys designated for fixed prostheses manufacture were selected for the experiments. Using cast plates, p...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Metallurgical and Materials Transactions A
سال: 1997
ISSN: 1073-5623,1543-1940
DOI: 10.1007/s11661-997-0051-4