Hydrogen embrittlement of cold-worked metastable austenitic stainless steels.
نویسندگان
چکیده
منابع مشابه
Delayed Cracking of Metastable Austenitic Stainless Steels after Deep Drawing
In metastable austenitic stainless steels, strain-induced martensitic transformation during plastic deformation enhances work hardening of the material, increasing its strength and in some cases also ductility.1,2) The presence of α’-martensite, however, may increase the susceptibility of these materials to hydrogen embrittlement phenomena, for example delayed cracking.3–6) Delayed cracking can...
متن کاملWarm Pre-Strain: Strengthening the Metastable 304L Austenitic Stainless Steel without Compromising Its Hydrogen Embrittlement Resistance
Plastic pre-strains were applied to the metastable 304L austenitic stainless steel at both room temperature (20 °C) and higher temperatures (i.e., 50, 80 and 100 °C), and then the hydrogen embrittlement (HE) susceptibility of the steel was evaluated by cathodically hydrogen-charging and tensile testing. The 20 °C pre-strain greatly strengthened the steel, but simultaneously significantly increa...
متن کاملLow-Temperature Carburization of Austenitic Stainless Steels
LOW-TEMPERATURE CARBURIZATION is a gaseous carburization process performed at atmospheric pressure, at temperatures where the kinetics of substitutional diffusion are very slow. Low-temperature carburization hardens the surface of austenitic stainless steels through the diffusion of interstitial carbon, without the formation of carbides. The surface must be activated, by modification and remova...
متن کاملDevelopment of Alumina-Forming Austenitic Stainless Steels
This paper presents the results of the continued development of creep-resistant, alumina-forming austenitic (AFA) stainless steel alloys, which exhibit a unique combination of excellent oxidation resistance via protective alumina (Al2O3) scale formation and high-temperature creep strength through the formation of stable nano-scale MC carbides and intermetallic precipitates. Efforts in fiscal ye...
متن کاملY Studies on Austenitic Stainless Steels
Abstract--In this investigation, the fracture surfaces of SS 304 and SS 316 austenitic steels were analysed using the X-ray fractography technique. In both cases, a decrease in the austenite content was observed at the fracture surface as a result of deformation induced martensite, indicating a linear relation with Km~ within the stable crack growth region. The presence of this martensite was f...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Society of Materials Science, Japan
سال: 1991
ISSN: 1880-7488,0514-5163
DOI: 10.2472/jsms.40.451