Hot nanoindentation in inert environments.
An instrument capable of performing nanoindentation at temperatures up to 500 degrees C in inert atmospheres, including partial vacuum and gas near atmospheric pressures, is described. Technical issues associated with the technique (such as drift and noise) and the instrument (such as tip erosion and radiative heating of the transducer) are identified and addressed. Based on these consideration...
متن کاملHot Nanoindentation of Nanocrystalline Ni-W Alloys
High temperature nanoindentation experiments are conducted to assess the activation enthalpy for deformation of nanocrystalline Ni-W alloys, for grain sizes between 3 and 80 nm. Thermal softening becomes less pronounced at finer grain sizes, and the activation enthalpy has an apparent inflection at a grain size near ~10-20 nm, in the vicinity the Hall-Petch breakdown. This inflection is related...
متن کاملProtective clothing in hot environments.
The high level of protection required by personal protective clothing (PPC) severely impedes heat exchange by sweat evaporation. As a result work associated with wearing PPC, particularly in hot environments, implies considerable physiological strain and may render workers exhausted in a short time. Recent development of algorithms for describing the heat transfer, accounting for pumping and wi...
متن کاملDyslipidemia in industrial workers in hot environments.
The aim of the study was to follow the rate and manifestation of dyslipidemia in industrial workers exposed to heat. One hundred and two male industrial workers exposed to heat and a control group of 102 male workers were studied. The microclimate components were followed and Wet Bulb Globe Temperature (WBGT) was calculated. The mean WGBT was 35.4 degrees C (28.4-41.7 degrees C) for the studied...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Review of Scientific Instruments
سال: 2010
ISSN: 0034-6748,1089-7623
DOI: 10.1063/1.3436633