Effect of Heat Treatment Process on Microstructure and Fatigue Behavior of a Nickel-Base Superalloy
The study of fatigue behaviors for nickel-base superalloys is very significant because fatigue damage results in serious consequences. In this paper, two kinds of heat treatment procedures (Pro.I and Pro.II) were taken to investigate the effect of heat treatment on microstructures and fatigue behaviors of a nickel-base superalloy. Fatigue behaviors were studied through total strain controlled m...
متن کاملHigh Temperature Deformation Mechanisms in a DLD Nickel Superalloy
The realisation of employing Additive Layer Manufacturing (ALM) technologies to produce components in the aerospace industry is significantly increasing. This can be attributed to their ability to offer the near-net shape fabrication of fully dense components with a high potential for geometrical optimisation, all of which contribute to subsequent reductions in material wastage and component we...
متن کاملJoining of nickel-base superalloy single crystals
Introduction ................................................................................................................................1 Overview of Weldability of Nickel-Base Superalloys..................................................................1 Crystallography............................................................................................................................
متن کاملOn APFIM of Grain Boundaries in a Nickel Base Superalloy
Experimental details of atom probe field ion microscopy (APFIM) of a Ni-16Cr-9Fe alloy are presented. In particular, studies concerning analysis of intergranular carbides and borides and segregation to grain boundaries are described. It was found that NiZ3B6 precipitates are very sensitive to preferential field evaporation, which necessitates optimization of the analysis conditions. In the FIM ...
متن کاملDesign of a nickel-base superalloy using a neural network
A new computational tool has been developed to model, discover, and optimize new alloys that simultaneously satisfy up to eleven physical criteria. An artificial neural network is trained from pre-existing materials data that enables the prediction of individual material properties both as a function of composition and heat treatment routine, which allows it to optimize the material properties ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Advanced Materials Research
سال: 2011
ISSN: 1662-8985
DOI: 10.4028/www.scientific.net/amr.278.411