Hot Corrosion of SrTiO3 Perovskite in Na2SO4 + 50 wt.% V2O5 and Na2SO4 + 10 wt.% NaCl Environments at 900°C

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effects of NaCl and Na2SO4 on germination and initial growth phase of Halostachys caspica

Current research on effect of increasing concentrations (0 (control), 100, 200, 300, 400 and 500 mM) of different salts including NaCl and Na2SO4 on germination and initial growth phase of Halostachys caspica were studied. The experimental design was completely randomized design with three replications. Characters of percentage, speed and index of germination, seed healthy index, radicle, plumu...

متن کامل

Effect of NaCl and Na2SO4 on the biodecolourization of K-2BP by Halomonas sp. GYW

In this paper, the effect of NaCl and Na2SO4 on the biodecolourization of reactive brilliant red K-2BP by a Halomonas sp. GYW (EF188281) was investigated in details. The decolourisation efficiency and the oxidation-reduction potential (ORP) change were explored during the decolourization process. The results from sequencing batch tests showed that Na2SO4 influenced the decolourization efficienc...

متن کامل

Comparison of Medium Manganese Steel and Q345 Steel on Corrosion Behavior in a 3.5 wt % NaCl Solution

A cyclic wet/dry accelerated corrosion test was used to compare the corrosion behavior of medium-Mn steel and Q345 steel. In terms of scanning electron microscope (SEM), using X-ray diffraction (XRD), electron probe microanalysis (EPMA), X-ray photoelectron spectroscopy (XPS), and analysis of the corrosion process, the results showed that the medium-Mn steel did not exhibit higher corrosion res...

متن کامل

The Corrosion Behavior of Pure Iron under Solid Na2SO4 Deposit in Wet Oxygen Flow at 500 °C

The corrosion behavior of pure Fe under a Na₂SO₄ deposit in an atmosphere of O₂ + H₂O was investigated at 500 °C by thermo gravimetric, and electrochemical measurements, viz. potentiodynamic polarization, electrochemical impedance spectroscopy (EIS), and surface characterization methods viz. X-ray diffraction (XRD), and scanning electron microscope (SEM)/energy dispersive spectroscopy(EDS). The...

متن کامل

Adiabatic calorimetric decomposition studies of 50 wt.% hydroxylamine/water.

Calorimetric data can provide a basis for determining potential hazards in reactions, storage, and transportation of process chemicals. This work provides calorimetric data for the thermal decomposition behavior in air of 50wt.% hydroxylamine/water (HA), both with and without added stabilizers, which was measured in closed cells with an automatic pressure tracking adiabatic calorimeter (APTAC)....

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: International Journal of Corrosion

سال: 2018

ISSN: 1687-9325,1687-9333

DOI: 10.1155/2018/4763085