Hot corrosions of laser-cladded inconel 625 in molten salt Na2SO4-MgSO4 mixture have been studied at 900 °C to address its anticorrosion behaviors. Elemental and microstructural characterizations provide direct evidence for the formation MgO/Cr2O3 external layers outward-diffusion Cr atoms. The Cr-depletion promotes precipitation δ-Ni3(Nb/Mo), nucleation accumulation dislocations, pores, internal spallation corroded alloy. They also diffusion sulfur into near-surface region, leading sulfide scales (i.e., Nb4−xCrxS6, CrS, MnCr2S4). Grain boundaries play important roles atomic diffusions formations.
منابع مشابه
Investigation on the Effect of Post Weld Heat Treatment Temperature on Stress Corrosion Resistance of Inconel 625 Cladded on AISI 4130 Steel Using Hot Wire GTAW
In this research the effect of heat treatment offer welding (PWHT) in 650,750 and 8500C for two hours on Sulfide stress corrosion cracking resistance (SSC), welding metal Inconel 625 to low alloy steel 4130 was analyzed that was welded using Automatic TIG welding process then the mechanical properties of the joint was observed using micro hardness measure experiment (weld metal, base metal and...
متن کاملInvestigation on the Effect of Post Weld Heat Treatment Temperature on Stress Corrosion Resistance of Inconel 625 Cladded on AISI 4130 Steel Using Hot Wire GTAW
In this research the effect of heat treatment offer welding (PWHT) in 650,750 and 8500C for two hours on Sulfide stress corrosion cracking resistance (SSC), welding metal Inconel 625 to low alloy steel 4130 was analyzed that was welded using Automatic TIG welding process then the mechanical properties of the joint was observed using micro hardness measure experiment (weld metal, base metal and...
متن کاملEvaluation of microstructure and corrosion behavior of dissimilar laser joint between Inconel 625 and AISI 430 ferritic stainless steel
Dissimilar weld joints between stainless steels and nickel based super alloys are extensively used in petrochemical, gas and oil applications. These joints jave great challenges from metallurgical transformations point of view. In this research, microstructural evolutions and corrosion behavior of laser weld joint between Inconel 625 and AISI 430 ferritic stainless steel were investigated. Ferr...
متن کاملEvaluation of microstructure and corrosion behavior of dissimilar laser joint between Inconel 625 and AISI 430 ferritic stainless steel
Dissimilar weld joints between stainless steels and nickel based super alloys are extensively used in petrochemical, gas and oil applications. These joints jave great challenges from metallurgical transformations point of view. In this research, microstructural evolutions and corrosion behavior of laser weld joint between Inconel 625 and AISI 430 ferritic stainless steel were investigated. Ferr...
متن کاملLaser clading of Inconel 625 on ASTM A575 steel
In this research, the microstructure of Inconel 625 cladded layer on ASTM A575 steel has been investigated. By examining different parameters, the optimal single-pass sample with the least amount of dilution, porosity and fusion and suitable wetting angle was determined. Then cladding process with the optimal parameter was performed. The microstructure of the cladding layer was evaluated from t...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Corrosion Science
سال: 2021
ISSN: ['1879-0496', '0010-938X']
DOI: https://doi.org/10.1016/j.corsci.2021.109869