Hot compression deformation behavior of extruded ZK61M magnesium alloy and establishment of constitutive equation
نویسندگان
چکیده
منابع مشابه
Constitutive Equation and Hot Compression Deformation Behavior of Homogenized Al–7.5Zn–1.5Mg–0.2Cu–0.2Zr Alloy
The deformation behavior of homogenized Al-7.5Zn-1.5Mg-0.2Cu-0.2Zr alloy has been studied by a set of isothermal hot compression tests, which were carried out over the temperature ranging from 350 °C to 450 °C and the strain rate ranging from 0.001 s-1 to 10 s-1 on Gleeble-3500 thermal simulation machine. The associated microstructure was studied using electron back scattered diffraction (EBSD)...
متن کاملA comparative study on constitutive modeling of hot deformation flow curves in AZ91 magnesium alloy
Modeling the flow curves of materials at elevated temperatures is the first step in mathematical simulation of the hot deformation processes of them. In this work a comparative study was provided to examine the capability of three different constitutive equations in modeling the hot deformation flow curves of AZ91 magnesium alloy. For this, the Arrhenius equation with strain dependent constants...
متن کاملHot Deformation Mechanisms in AZ31 Magnesium Alloy Extruded at Different Temperatures: Impact of Texture
The hot deformation characteristics of AZ31 magnesium alloy rod extruded at temperatures of 300 °C, 350 °C and 450 °C have been studied in compression. The extruded material had a fiber texture with > < 0 1 10 parallel to the extrusion axis. When extruded at 450 °C, the texture was less intense and the > < 0 1 10 direction moved away from the extrusion axis. The processing maps for the material...
متن کاملGrain Refinement and Enhancement of Mechanical Properties of Hot Extruded Rare-Earth Containing Magnesium Alloy
The effects of rare earth addition and hot extrusion process on the grain refinement of magnesium alloy were studied. The as-cast Mg-6Al-1Zn (AZ61) alloy had the average grain size of ~ 64 µm and its microstructure consisted of α-Mg and Mg17Al12 phase. By partial substitution of Al with Gd to reach Mg-4.8Gd-1.2Al-1Zn alloy, it was observed that the Mg17Al12 phase disappeared and two new interme...
متن کاملTHE DEFORMATION BEHAVIOR OF AZ31 MAGNESIUM ALLOY AT ELEVATED TEMPERATURES
AZ31 magnesium alloy is considered as a promising alloy in various applications and industries. Furthermore, to design a proper hot working process (rolling, forging and extrusion), the assessment of hot working behaviour of the alloy is necessary. Accordingly, the hot deformation behaviour of AZ31 alloy was studied through hot compression testing method This was carried out in a wide range of ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Procedia Manufacturing
سال: 2020
ISSN: 2351-9789
DOI: 10.1016/j.promfg.2020.08.114