High-Temperature Tensile Properties of a Cobalt-Based Co-20Cr-15W-10Ni Superalloy with a Bimodal Grain Structure

نویسندگان

چکیده

Cobalt-based superalloys are common materials for the manufacturing of various components used in aerospace applications. Conventional cobalt-based with a unimodal grain structure generally exhibit low strength and ductility at high temperatures. A bimodal superalloy, Co–20Cr–15W–10Ni (CCWN), was designed to achieve both The deformation behavior tensile properties CCWN alloy fine-grain (FG), coarse-grain (CG), (FG/CG) structures were investigated 900 °C. microstructures substructures after high-temperature examined via electron backscatter diffraction (EBSD) channeling contrast imaging (ECCI) determine mechanisms. microstructural observation showed that consisted FG CG domains. During °C, mainly deformed by dynamic recrystallization (DRX), maintaining similar structure. DRV, resulting small amount DRX grains large recovery (DRV) grains. However, softened transformed into new structure, ultrafine (UFG) FG. domains tended deform dislocations, twinning. tests revealed bimodal-structured exhibited higher than those samples or This is associated newly developed UFG/FG grain-structured during deformation. work may provide insight development alloys structures.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

High-temperature tensile properties of a polymer intercalated/exfoliated cement

A polymer intercalated/exfoliated (PIE) cement is synthesized and its high-temperature tensile performance is characterized. Due to the reinforcing effect of the nanointerphase, the flexure strength of the PIE cement is higher than that of ordinary cements by more than an order of magnitude in a broad temperature range. The temperature at which the optimum mechanical properties are obtained is ...

متن کامل

Influence of Solidification Conditions on TCP Phase Formation, Casting Porosity and High Temperature Mechanical Properties in a Re-Containing Nickel-Base Superalloy with Columnar Grain Structure

A coarse and a fine dendrite structure were produced using the newly developed DS-superalloy ExAl7 ( IN792 with 2-3 wt.-% Re) by changing the conditions of directional solidification. The two microstructures differed in their primary dendrite arm spacing by a factor of 1.6. During aging, very fine TCP phase precipitates (length approximately 20 m, volume fraction ~ 1 %) were precipitated in the...

متن کامل

construction and validation of a computerized adaptive translation test (a receptive based study)

آزمون انطباقی رایانه ای (cat) روشی نوین برای سنجش سطح علمی دانش آموزان می باشد. در حقیقت آزمون های رایانه ای با سرعت بالایی به سمت و سوی جایگزین عملی برای آزمون های کاغذی می روند (کینگزبری، هاوسر، 1993). مقاله حاضر به دنبال آزمون انطباقی رایانه ای برای ترجمه می باشد. بدین منظور دو پرسشنامه مشتمل بر 55 تست ترجمه میان 102 آزمودنی و 10 مدرس زبان انگلیسی پخش گردید. پرسشنامه اول میان 102 دانشجوی س...

Effect of high temperature deformation on the structure of Ni based superalloy

Purpose: A study on the hot deformation behaviour and dynamic structural processes (dynamic precipitation operating during deformation at elevated temperatures) of nickel based superalloy was presented. Design/methodology/approach: Compression tests were carried out on precipitations hardenable nickel based superalloy of Inconel 718 at constant true strain rates of 10-4, 4x10-4s-1 within a temp...

متن کامل

HIGH TEMPERATURE TENSILE PROPERTIES OF NEW FE-CR-MN DEVELOPED STEEL

Nowadays, Ni-free austenitic stainless steels are being developed rapidly and high price of nickel is one of the most important motivations for this development. At present research a new FeCrMn steel was designed and produced based on Fe-Cr-Mn-C system. Comparative studies on microstructure and high temperature mechanical properties of  new steel and AISI 316 steel were done. The results ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Crystals

سال: 2023

ISSN: ['2073-4352']

DOI: https://doi.org/10.3390/cryst13020232