High Temperature Strength. Diffusion Bonding between Ni-Base ODS Alloy and Conventional Ni-Base Superalloy and High-Temperature Fatigue Strength of the Joints.
نویسندگان
چکیده
منابع مشابه
High Temperature Nanoindentation of Ni-base Superalloys
Novel techniques for characterizing and assessing the properties of Ni-base superalloys are becoming increasingly important to the accelerated development of new structural alloys and the advancement of physics-based mechanical property models. Instrumented indentation techniques have long served as a useful approach for probing the mechanical response of a wide range of engineering materials. ...
متن کاملThermomechanical Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy
A continuum crystal plasticity model is used to simulate the material behavior of a directionally solidified Ni-base superalloy, DS GTD-111, in the longitudinal and transverse orientations. Isothermal uniaxial fatigue tests with hold times and creep tests are conducted at temperatures ranging from room temperature (RT) to 1038°C to characterize the deformation response. The constitutive model i...
متن کاملVery High Cycle Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy DZ4
The effect of casting pores on the very high cycle fatigue (VHCF) behavior of a directionally solidified (DS) Ni-base superalloy DZ4 is investigated. Casting and hot isostatic pressing (HIP) specimens were subjected to very high cycle fatigue loading in an ambient atmosphere. The results demonstrated that the continuously descending S-N curves were exhibited for both the casting and HIP specime...
متن کاملModeling the Temperature-dependence of Tertiary Creep Damage of a Directionally Solidified Ni-base Superalloy
Directionally solidified (DS) Ni-base superalloys have become a commonly used material in gas turbine components. Controlled solidification during the material manufacturing process leads to a special alignment of the grain boundaries within the material. This alignment results in different material properties dependent on the orientation of the material. When used in gas turbine applications t...
متن کاملFretting on the cubic face of a single-crystal Ni-base superalloy at room temperature
Fretting experiments were conducted on the (10 0) crystal (cubic) face of a single crystal Ni-base superalloy in two directions, /10 0S and /110S, to study the effect of crystallographic orientation on the fretting response in both partial slip and gross slip regimes. The study involved point contacts using a tungsten carbide (WC) ball with radius 10 mm tested at room temperature. Ball indentat...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Society of Materials Science, Japan
سال: 2001
ISSN: 1880-7488,0514-5163
DOI: 10.2472/jsms.50.144