High-performance IN738 superalloy derived from turbine blade waste for efficient ethanol, ethylene glycol, and urea electrooxidation

نویسندگان

چکیده

Abstract In this work, IN738 superalloy used previously in gas turbines was recycled and as a working electrode for the electrooxidation of different fuels, namely ethylene glycol, ethanol, urea. The electrocatalytic efficiency studied by cyclic voltammetry, chronoamperometry, electrochemical impedance. Several kinetics parameters like diffusion coefficient, Tafel slope, rate constant, activation energy were calculated. modified characterized received using XRD, SEM, EDAX to elucidate crystal structure surface morphology before after oxidation. anodic current densities oxidation urea 29, 17, 12 mA.cm ?2 , respectively, an alkaline solution at potential 0.6 V (vs. Ag/AgCl). kinetic coefficients found be 1.5 $$\times$$ × 10 –6 1.038 0.64 cm 2 s ?1 respectively. charge transfer resistances estimated fuels impedance spectroscopy (EIS). Graphical

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Treatment of Waste Water Containing Ethylene Glycol using Ozonation: Kinetic and Performance Study

Ethylene Glycol (EG) is one of toxic and hazardous materials that was used in many industries such as; synthetic fibers, films, antifreeze, resins, explosives, fibers, paper, leather, protective coatings, printing inks and textile. Many environmental problems such as: negative effects on aquatic life, destruction of aquatic ecosystems, soil pollution, reducing the oxygenlevel in the waterabsorp...

متن کامل

Tough high modulus hydrogels derived from carbon-nitride via an ethylene glycol co-solvent route.

High concentration formulations of graphitic carbon nitride (g-CN) are utilized as photoinitiator and reinforcer for hydrogels. In order to integrate significant amounts of g-CN, ethylene glycol (EG) is employed as a co-solvent for the gel formation, which enables stable dispersion of up to 4 wt% g-CN. Afterwards, EG can be removed easily via solvent exchange to afford pure hydrogels. The diver...

متن کامل

Blade Design and Performance Analysis of Wind Turbine

This paper reviews the design optimization of wind turbine blades through investigating the design methods and analyzing the performance of the blades. The current research work in this area include wind turbine blade geometric design and optimization, aerodynamics analysis, wind turbine blade structural design and dynamics analysis. Blade geometric design addresses the design parameters, inclu...

متن کامل

Electrocatalytic Oxidation of Ethanol and Ethylene Glycol onto Poly (o-Anisidine)-Nickel Composite Electrode

In this work, poly (o-Anisidine) (POA) was prepared by consecutive potential cycling in an acidic monomer solution at the surface of Carbon Paste Electrode (CPE). Nickel ions were dispersed into the polymer by immersing the electrode in NiSO4 solution. The prepared Ni/POA/CPE was characterized by scanning electron microscopy, energy dispersive X-ray spectroscopy, Atomic Force Mic...

متن کامل

Turbine Blade Illusion

In January 2017, a large wind turbine blade was installed temporarily in a city square as a public artwork. At first sight, media photographs of the installation appeared to be fakes - the blade looks like it could not really be part of the scene. Close inspection of the object shows that its paradoxical visual appearance can be attributed to unconscious assumptions about object shape and light...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Applied Electrochemistry

سال: 2023

ISSN: ['1572-8838', '0021-891X']

DOI: https://doi.org/10.1007/s10800-023-01862-7