EVect of high energy ball milling on titanium– hydroxyapatite powders
to bone are concerned are brittle materials as exempli ed by hydroxyapatite and ‘Bioglass’. Bioactive coatings are This paper reports on an investigationof the potential employed on metal implants to facilitate bonding to bone use of high energy ball milling (HEBM) for the while retaining the good combination of mechanical production of homogeneous mixtures of titanium/ properties associated w...
متن کاملSintering and Characterizations of WC-20wt.% (Fe,Co) Nano-Structured Powders Developed by Ball-Milling
The aim of the present work is to study the effects of the nanostructured WC-20 wt. % (Fe,Co) with different ratios of iron to cobalt on the microstructure and hardness of sintered samples. Furthermore, a sample with a cobalt binder under the same condition was produced for the comparison purposes. The nanocomposite development, after different milling times, has been monitored by means of X-ra...
متن کاملEffect of High-Energy Ball Milling on the Magnetic Properties of NiZn Ferrite Ceramics Synthesized by Spark Plasma Sintering
High-density fine-grained Ni0.5Zn0.5Fe2O4 ferrite ceramics were synthesized by spark plasma sintering (SPS) in conjunction with high energy ball milling. The precursor powders were milled for 20 h, 40 h, and 60 h, respectively, and the milled powders were all sintered for 5 min at 900 ̊C. All the samples exhibit a single spinel phase. With increasing of the ball milling time, the relative densit...
متن کاملFabrication of Nanostructured Cu matrix Nanocomposites by High Energy Mechanical Milling and Spark Plasma Sintering
Spark plasma sintering (SPS) is a sintering process that is capable of sintering hard worked powders in short times. This technique was used to fabricate bulk Cu and Cu-SiC nanocomposites. Pure Cu and mixed powders of Cu including 4 vol% of SiC nanoparticles were mechanically alloyed for 25 h and sintered at 750˚C under vacuum condition by SPS method. Microstructures of the materials were chara...
متن کاملFormation of glassy Ti50Cu20Ni24Si4B2 alloy by high-energy ball milling
The elemental powder mixtures with a nominal composition of Ti50Cu20Ni24Si4B2 can be amorphized under high-energy ball milling. A well-defined glass transition before crystallization appears in the obtained amorphous phase during heating in a differential scanning calorimeter. Awide supercooled liquid region DTx is available to be about 57 K. Crystallization of the ballmilled amorphous phase wa...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Acta Physica Polonica A
سال: 2017
ISSN: 0587-4246,1898-794X
DOI: 10.12693/aphyspola.131.329