High cycle thermal fatigue of austenitic stainless steel
نویسندگان
چکیده
منابع مشابه
Fatigue behavior of Austenitic Type 316L Stainless Steel
The aim of this work is to determine the fatigue life of 316L stainless steel. The mechanisms of fatigue of 316L stainless steels were investigated and discussed. The fatigue tests were carried out at constant-amplitude cyclic loading with load ratio R=0.1. Scanning Electron Microscope (SEM) is then used to examine the fracture surface. The results show that the fatigue limit of 316L stainless ...
متن کاملUltrasonic Characterization of Austenitic Stainless Steel in Thermal Variations
This work focuses on the ultrasonic characterization and hardness of Austenitic stainless steel in thermal variation. The sample which was heat treated at 1050 o C has the highest hardness value and plays a dominant role in dispersion of carbides. Shear wave velocity and hardness show similar trend in variation with temperature. The effect of volume expansion would be to decrease the elastic co...
متن کاملEnergy-Based Prediction of Low-Cycle Fatigue Life of CK45 Steel and SS316 Stainless Steel
In this paper, low cycle fatigue life of CK45 steel and SS316 stainless steel under strain-controlled loading are experimentally investigated. In addition, the impact of mean strain and strain amplitude on the fatigue life and cyclic behavior of the materials are studied. Furthermore, it is attempted to predict fatigue life using energy and SWT damage parameters. The experimental results demons...
متن کاملCreep and Fatigue Interaction Behavior in Sanicro 25 Heat Resistant Austenitic Stainless Steel
Sanicro 25 is a newly developed advanced high strength heat resistant austenitic stainless steel. The material shows good resistance to steam oxidation and flue gas corrosion, and has higher creep rupture strength than other austenitic stainless steels available today. It is thus an excellent candidate for superheaters and reheaters for advanced ultra-super critical power plants with efficiency...
متن کاملSensitization Behavior of Gnaw Austenitic Stainless Steel Joints
The present work has been carried out to study the sensitization behavior of AISI 304L austenitic stainless steel weld, fabricated using GTAW (gas tungsten arc welding process). This weld was subjected to post weld thermal aging (PWTA) treatments lying in the sensitization range, viz. 700 ?C for 30 minutes, 500 minutes and 1000 minutes for studying the influence of carbide precipitation on thei...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: MATEC Web of Conferences
سال: 2018
ISSN: 2261-236X
DOI: 10.1051/matecconf/201816519009