Hardness and Fracture Toughness of Commercial Core Composite Resins

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Marginal fracture toughness of composite resins.

The marginal fracture toughness of several types of composite resins was determined by means of the rattler test. Microparticle-filled resins showed significantly higher marginal fracture toughness than conventional composites. Posterior restorative composites were intermediate between MFRs and conventional composites. Amalgams were inferior to restorative resins. These data correspond with the...

متن کامل

Fracture toughness of composite and unfilled restorative resins.

Fracture toughness, critical strain energy release rate, and critical stress intensity factor were determined for experimental and commercial restorative resins. A composite resin had lower resistance to crack initiation than an unfilled acrylic resin. The data were consistent with surface failure observed in single-pass wear studies of these resins.

متن کامل

On the velocity-dependent fracture toughness of epoxy resins

In a recent paper [1], Drs Selby and Miller described three methods of determining the fracture toughness (R), or equivalently, the fracture surface energy (23') for an epoxy resin. These methods are respectively (a) Berry's method, (b) Irwin-Kies equation and (c) Gurney's irreversible work area method. While the experimental data obtained from tapered double-cantilever beam (TDCB) specimens su...

متن کامل

Hardness Evaluation of Composite Resins Cured with QTH and LED

UNLABELLED Background and aims. Today light cured composites are widely used. Physical and mechanical properties of composites are related to the degree of conversion. Light curing unit (LCU) is an important factor for composite polymerization. Aim of this study is evaluation of composite resins hardness using halogen and LED light curing units. Materials and methods. In this study, 30 samples ...

متن کامل

Evaluation of brittleness of porcelain fused to pure titanium by fracture toughness, hardness and fracture energy.

To elucidate the cause of brittleness of porcelain fused to pure titanium (PFPT) which leads to chipping and cracking similar to that of conventional porcelain in clinical use, fracture toughness KIc, hardness (Hv and Hk) and fracture energy gamma reflecting the bonding energy of atoms were evaluated. In KIc there were no differences between PFPT and conventional porcelain, nor for Hv and Hk, b...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Dental Materials Journal

سال: 1993

ISSN: 1881-1361,0287-4547

DOI: 10.4012/dmj.12.62