Grindability and Surface Integrity of Cast Nickel-based Superalloy in Creep Feed Grinding with Brazed CBN Abrasive Wheels
نویسندگان
چکیده
منابع مشابه
Investigation into Grindability of Gh4169 Superalloy and Effects of Grinding Parameters on the Surface Integrity
GH4169, a nickel-base heat-resistant alloy, usually has outstanding high-temperature strength, excellent thermal stability and good wear resistance. However, it is hard to cut and its machined surface quality and integrity are particularly sensitive to a manufacturing process employed. The study reported in this paper was conducted to initially, review existing research on machining-induced sur...
متن کاملA Study on Fracture Behavior of Brazed Multicrystalline CBN Abrasive Grains During Grinding
This paper analyses the fracture behavior of the brazed BCBN grain by comparison with brazed PCBN grain through grinding test of Nickel-based superalloy. The self-sharpening effect is created by timing micro-fracture behavior for BCBN abrasive grains, but by macro-fracture behavior for PCBN abrasive grains. During grinding with brazed BCBN abrasive grains, the material is removed together with ...
متن کاملUltrasonic assisted creep feed grinding of Inconel
The paper details the effects of depth of cut and vibration amplitude when ultrasonic assisted (US) creep feed grinding Inconel 718 with an open structured alumina based wheel. The workpiece was actuated at a constant frequency (~20.5kHz) via a block sonotrode attached to a 1kW piezoelectric transducer-generator system. A full factorial experimental array comprising 12 tests was conducted invol...
متن کاملFractal Analysis of Micro Self-Sharpening Phenomenon in Grinding with Cubic Boron Nitride (cBN) Wheels
متن کامل
Ultrasonic assisted creep feed grinding of Inconel 718
The paper details the effects of depth of cut and vibration amplitude when ultrasonic assisted (US) creep feed grinding Inconel 718 with an open structured alumina based wheel. The workpiece was actuated at a constant frequency (~20.5kHz) via a block sonotrode attached to a 1kW piezoelectric transducer-generator system. A full factorial experimental array comprising 12 tests was conducted invol...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Chinese Journal of Aeronautics
سال: 2010
ISSN: 1000-9361
DOI: 10.1016/s1000-9361(09)60247-8