Grain refining of Ti-6Al-4V alloy fabricated by laser and wire additive manufacturing assisted with ultrasonic vibration
نویسندگان
چکیده
منابع مشابه
Residual Stress, Defects and Grain Morphology of Ti-6Al-4V Alloy Produced by Ultrasonic Impact Treatment Assisted Selective Laser Melting
For large-scale selective laser melting (SLM) additive manufacturing technology, three main problems severely restrict its development and application, namely the residual stress, defects, and columnar grains with anisotropy. To overcome these problems, a new method is proposed by combining SLM with ultrasonic impact treatment (UIT) technique. This study explores the feasibility of UIT assisted...
متن کاملEffect of Molten Pool Size on Microstructure and Tensile Properties of Wire Arc Additive Manufacturing of Ti-6Al-4V Alloy
Wire arc additive manufacturing (WAAM) technique is a cost-competitive and efficient technology to produce large structure components in industry domains. Mechanical properties are mainly dominated by the microstructure of the components, which is deeply affected by the molten pool size. In this work, to investigate the effect of the molten pool size on microstructure and mechanical properties ...
متن کاملLaser Powder Cladding of Ti-6Al-4V α/β Alloy
Laser cladding process was performed on a commercial Ti-6Al-4V (α + β) titanium alloy by means of tungsten carbide-nickel based alloy powder blend. Nd:YAG laser with a 2.2-KW continuous wave was used with coaxial jet nozzle coupled with a standard powder feeding system. Four-track deposition of a blended powder consisting of 60 wt % tungsten carbide (WC) and 40 wt % NiCrBSi was successfully mad...
متن کاملMicrostructure and Mechanical Properties of Ti-6Al-4V Fabricated by Vertical Wire Feeding with Axisymmetric Multi-Laser Source
Vertical wire feeding with an axisymmetric multi-laser source (feeding the wire vertically into the molten pool) has exhibited great advantages over LAM (laser additive manufacturing) with paraxial wire feeding, which has an anisotropic forming problem in different scanning directions. This paper investigates the forming ability of vertical wire feeding with an axisymmetric multi-laser source, ...
متن کاملAdditive Manufacturing Laser Deposition of Ti-6Al-4V for Aerospace Repair Applications
Parts or products from high performance metal are very expensive, partly due to the processing complexities during manufacturing. The purpose of this project is to use additive laser deposition and machining processes to repair titanium parts, thus extending the service life of these parts. The study broadly included preparing the defects, laser deposition, machining, sample preparation and mec...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Ultrasonics Sonochemistry
سال: 2021
ISSN: 1350-4177
DOI: 10.1016/j.ultsonch.2021.105472