Grain refinement of TiAl alloys by isomorphic self-inoculation
نویسندگان
چکیده
منابع مشابه
Magnificent Grain Refinement of Al-Mg2Si Composite by Hot Rolling
The effect of chemical composition and the hot rolling operations on the microstructure and mechanical properties of in situ aluminum matrix composite with Mg2Si phase as the reinforcement was studied. It was revealed that the modification by phosphorous results in the rounder (more spherical) primary and secondary (eutectic) magnesium silicide intermetallics. During hot rolling, the primary pa...
متن کاملATOMISTIC STUDIES OF JOGGED SCREW DISLOCATIONS IN y-TIAL ALLOYS
The behavior of jogged screw dislocations in y-TiAl alloys has been investigated with large-scale molecular dynamics (MD) simuIations. We find a new mechanism for formation of pinning points in jogged screw dislocations. We also find that the critical height for the jogs in the +[i10] directions on the (001) plane to move nonconservatively is between 3ro and 4r0, where ro is the nearest neighbo...
متن کاملGrain Refinement Efficiency in Commercial-Purity Aluminum Influenced by the Addition of Al-4Ti Master Alloys with Varying TiAl3 Particles
A series of Al-4Ti master alloys with various TiAl₃ particles were prepared via pouring the pure aluminum added with K₂TiF₆ or sponge titanium into three different molds made of graphite, copper, and sand. The microstructure and morphology of TiAl₃ particles were characterized and analyzed by scanning electron microscope (SEM) with energy dispersive spectroscopy (EDS). The microstructure of TiA...
متن کاملThermal-cycling creep of g-TiAl-based alloys
In two-phase TiAl-based alloys, the coexisting 2 and phases exhibit a thermal expansion mismatch, so that increased creep rates during thermal cycling may be expected. Creep deformation of two g-TiAl-based alloys was investigated during thermal cycles between 900 and 300 or 350 C with applied tensile stresses of 32.5 or 37.0 MPa. Measured thermal cycling creep rates were compared with isotherma...
متن کاملSuperplastic behaviour and mechanical properties of two phase TiAl alloys
High temperature plastic flow properties of two phase TiAl alloys containing 45 to 49 at.%Al have been investigated in thermo-mechanically grain refined materials in order to clarify the favourable microstructure and chemical composition for TiAl based superplastic materials. Grain sizes of thermomechanical treated materials and their grain size stability during subsequent high temperature defo...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Intermetallics
سال: 2018
ISSN: 0966-9795
DOI: 10.1016/j.intermet.2018.02.001