We investigated film thickness effects of sulfuric acid anodized aluminum when galvanically coupled with carbon fiber reinforced plastic(CFRP). The CFRP was electrically to alloys 1050, 5052, 6061, and 7075 in 3.5 wt.% NaCl solution at 35 ℃. Galvanic current passing from the 1050 6061 decreased as anodic oxide thickened. For galvanic between 5052 CFRP, elapsed time until corrosion density value increased tended increase passed irrespective thickness.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Dynamic Characteristics of Joined Steel and Carbon Fiber-Reinforced Plastic Tubes: Experimental and Numerical Investigation

The fundamental frequencies and mode shapes of steel and carbon fiber–reinforced plastic (CFRP) cylindrical shells with steel inserts were investigated using finite element analysis and modal testing. The free-free boundary condition was tested with modal testing using the roving hammer method and verified by finite element analysis using ABAQUS. The results show good agreement between the test...

متن کامل

Nanoporous anodized aluminum thickness optimization through pulse current mode

The purpose of this study was to optimize the thickness of anodizing Aluminum coatings processed under pulse current mode through the Design of Experiments (DOE) method. Thickness measurement, polarization and electrochemical impedance spectroscopy were employed to take Thickness and corrosion behaviors of the anodized coatings into consideration. Also, Field-emission scanning electron microsco...

متن کامل

Fiber reinforced plastic composites using recycled materials

This work investigates the feasibility of using recycled high density polyethylene (rHDPE), recycled polypropylene (rPP) and old newsprint fiber (ONP) to manufacture fiber reinforced composites. The boards were made through air-forming and hot press. The effects of the fiber loading and coupling agent content on tensile, flexural, internal bond properties and water absorption and thickness swel...

متن کامل

Corrosion of Thin Film Magnetic Disk: Galvanic Effects of the Carbon Overcoat

Thin film magnetic disks are usually coated with a layer of carbon or silica to improve wear properties, enhance flyability, and reduce environmental degradation of the underlying metal layers. In this paper we investigated the effect of dc and RF sputter deposited carbon overcoats on the corrosion behavior of the magnetic layers using electrochemical techniques and a corrosive gas chamber. Cor...

متن کامل

Bond Development Between Carbon Fiber Reinforced Polymers and Concrete

Carbon fiber reinforced polymer (CFRP) sheets can be externally bonded for retrofit of concrete structures, improving flexure and sheer strength in the concrete. The key to CFRP sheets is the bond to the concrete, as bond is the means to transfer stress between the tow sheet and the concrete. Experimentation has been conducted to test a current market fiber-resin system, and to develop a resin ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of The Surface Finishing Society of Japan

سال: 2022

ISSN: ['1884-3409', '0915-1869']

DOI: https://doi.org/10.4139/sfj.73.451