Galvanic Corrosion and Anodic Dissolution of Fe and Fe-Al Alloys.
نویسندگان
چکیده
منابع مشابه
CALCULATION OF THERMODYNAMIC PROPERTIES OF Al-Fe, Al-Ni AND Ni-Fe ALLOYS USING FACTSAGE
Thermodynamic predicting analysis of three binary systems Al-Fe, Al-Ni and Ni-Fe are shown in this paper. Thermodynamic analysis involved calculation of activities, coefficient of activities, partial and integral values for enthalpies and Gibbs energies of mixing and excess energies at three different temperatures: 1873K, 1900K and 1973K, as well as calculated phase diagrams, for the investigat...
متن کاملAtomistic Study of Surfaces and Interfaces of Fe-Cr and Fe-Cr-Al Alloys
Surface and interface properties of Fe-Cr, Fe-Al, and Fe-Cr-Al are studied using Exact Muffin-Tin Orbitals and Monte Carlo methods and with x-ray photoelectron and Auger electron techniques. Surface composition is investigated as a function of oxidation (heating) time. Hard x ray photoelectron spectroscopy (HAXPES) is used to scan non destructively the compositions below the surface. It is foun...
متن کاملGalvanic Corrosion Behavior of Dental Alloys
There is a wide variety of dental alloys, ranging from nearly pure gold and conventional gold-based alloys to alloys based on silver, palladium, nickel, cobalt, iron, titanium, tin, and other metals (Table 1). The types of dental alloys have increased significantly since 1980s in order to change the market price of gold and palladium. Although gold alloys are the mate‐ rials of choice in this a...
متن کاملpreparation and characterization of new co-fe and fe-mn nano catalysts using resol phenolic resin and response surface methodology study for fischer-tropsch synthesis
کاتالیزورهای co-fe-resol/sio2و fe-mn-resol/sio2 با استفاده از روش ساده و ارزان قیمت همرسوبی تهیه شدند. از رزین پلیمری resol در فرآیند تهیه کاتالیزور استفاده شد.
Composition, Morphology, and Topography of Galvanic Coatings Fe-Co-W and Fe-Co-Mo
Ternary coatings Fe-Co-W with an iron content of 40-55 at.%, cobalt 39-44 at.%, and tungsten 4-12 at.% and Fe-Co-Mo with an iron content of 40-55 at.%, cobalt 39-44 at.%, and tungsten 4-12 at.% were obtained by galvanostatic and pulse electrolysis on the mild steel substrate from iron(III) citrate-based electrolyte. The influence of electrolysis mode and parameters on composition of deposited a...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Surface Finishing Society of Japan
سال: 2002
ISSN: 0915-1869,1884-3409
DOI: 10.4139/sfj.53.618