Functionalization of Calcium Sulfate/Bioglass Scaffolds with Zinc Oxide Whisker.
There are urgent demands for satisfactory antibacterial activity and mechanical properties of bone scaffolds. In this study, zinc oxide whisker (ZnOw) was introduced into calcium sulfate/bioglass scaffolds. Antimicrobial behavior was analyzed using Escherichia coli (E. coli) and Staphylococcus aureus (S. aureus). The results showed that the scaffolds presented a strong antibacterial activity af...
متن کاملSynthesis of calcium carbide-derived carbon by mechanochemical reaction of calcium carbide with sulfur, iron sulfide and zinc oxide
In the present work, we report a novel design and preparation for the mechanochemical synthesis of calcium carbide-derived carbon (CaC2-CDC) at ambient temperature. Thermodynamic calculations confirmed the possibility of calcium carbide-derived carbon formation by the reaction of calcium carbide with sulfur, iron sulfide and zinc oxide at ambient temperature. The CDCs were synthesized by the ba...
متن کاملHydroxyapatite whisker-reinforced polyetherketoneketone bone ingrowth scaffolds.
Hydroxyapatite (HA) whisker-reinforced polyetherketoneketone (PEKK) bone ingrowth scaffolds were prepared and characterized. High levels of porosity (75-90%) and HA whisker reinforcement (0-40 vol.%) were attained using a powder processing approach to mix the HA whiskers, PEKK powder and a NaCl porogen, followed by compression molding at 350-375 degrees Celsius and particle leaching to remove t...
متن کاملSynthesis and study of co-doped zinc oxide nanoparticles with copper, magnesium, calcium, and cobalt ions by microemulsion method
In the present study, zinc oxide nanoparticles were synthesized by simultaneous doping of Zn0.98Cu0.02O with Ca2+, Mg2+, and Co2+ ions using the microemulsion method. The phase, crystallization, and particle size of samples were identified by X-ray diffraction (XRD) analysis. The formation of the desired phase was confirmed by, X-ray diffraction. Also, the infrared spectrum (Far-FTIR) was confi...
متن کاملPreparation of Cobalt Oxide/Zinc Oxide Nanocomposite
Cobalt Oxide/ Zinc Oxide nanocomposite was synthesized by dropwise addition ofCo(NO)3.6H2O and Zn(NO3)2.4H2O solutions to KOH solution at different temperatures followed bycalcination at 300ºC for 4 h. The morphology and structure of nanoparticles and the influence oftemperature on particle size were studied using scanning electron microscopy (SEM) and X-RayDiffraction (XRD). Minimum particle s...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Molecules
سال: 2016
ISSN: 1420-3049
DOI: 10.3390/molecules21030378