Carbide Structure and Fracture Toughness of High Speed Tool Steels
In the present study, M2 high speed steels were fabricated by using electro-slag rapid remelting process. Carbide structure was analysed and the fracture toughness and hardness were also measured after austenitization treatment at 1190 and 1210C followed by tempering treatment at 535C for billets with various diameters from 16 to 60 mm. Electro-slag rapid remelting (ESRR) process is an advanced...
متن کاملAnalysis of fracture resistance of tool steels by means of Acoustic Emission
The usage of advanced high strength steels (AHSS) in structural automotive components has been broadened in the past few years to satisfy the strict specifications of the automotive industry. Besides showing excellent strength to weight rations, AHSS have several limitations due to the high loads required in cold forming and cutting tools, which decrease considerably the tooling performances. T...
متن کاملMezzo-scopic Analysis of Fracture Toughness in Steels
The cleavage fracture toughness of steels was mezzo-scopically analyzed on the basis of the statistical local fracture criterion approach. The statistical stress criterion at the crack tip region suggests that the cleavage fracture toughness in steels can be described as a function of the yield stress, the cleavage fracture stress, and other mechanical properties of the materials. Formulation o...
متن کاملCreep Fracture in Tempered Martensitic Steels
Creep strength enhanced ferritic (CSEF) steels which contain 9 to 12%Cr have become the steels of choice in many industrial high energy systems. The typical compositions of alloy types P91, P92 and E911 are compared with 12CrMoV in Table 1. These steels are selected for use in applications where high temperature creep can occur because of a favorable balance between cost and properties [1,2]. T...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: ISRN Materials Science
سال: 2014
ISSN: 2090-6099
DOI: 10.1155/2014/489487