Mode I Interlaminar Fracture Toughness of Natural Fiber Stitched Flax/Epoxy Composite Laminates – Experimental and Numerical Analysis
The mode I interlaminar fracture toughness of stitched and unstitched composite laminates of continuous UD flax fiber and epoxy matrix was experimentally and numerically investigated. A twistless flax fiber yarn was used for stitching purpose. The mode I interlaminar energy release rate of the unstitched and stitched laminates was experimentally determined through Double Cantilever Beam (DCB) t...
متن کاملEffect of Rock Fracture Filling on Mode I and II Fracture Toughness
This paper focuses on some fracture toughness tests performed on the pre-cracked Brazilian specimens of rock-like materials. Also the effect of rock fracture filling on the fracture toughness was considered experimentally. Fracture toughness is a key parameter for studying the crack propagation and fragmentation processes in rock structures. Fracture mechanics is an applicable tool to improve ...
متن کاملPrediction of Mode II of Fracture Toughness in Laminate Composites
In this paper, effects of ply orientation of adjacent plies with (ϕ//θ) interfaces on mode II critical strain energy release rate (fracture toughness) of multidirectional (MD) laminate has been studied. Ply orientation of adjacent plies is one of the most important parameters affects the mode II critical strain energy release rate () in the initiation of the delamination. To study this paramet...
متن کاملMode I Interlaminar Fracture Toughness of Unidirectional Fiber-Reinforced Polymer Matrix Composites
1.1 This test method describes the determination of the opening Mode I interlaminar fracture toughness, GIc, of continuous fiber-reinforced composite materials using the double cantilever beam (DCB) specimen (Fig. 1). 1.2 This test method is limited to use with composites consisting of unidirectional carbon fiber and glass fiber tape laminates with brittle and tough single-phase polymer matrice...
متن کاملInterlaminar Mode II Fracture Characterization
Delamination is an important concern in the context of structural behaviour of laminated composite materials. It is known that delamination can diminish the stiffness and the strength of the material and promote structural failure. Delamination onset and growth is governed by interlaminar fracture toughness of the material. Delamination propagation is frequently dominated by mode II fracture; c...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: TRANSACTIONS OF THE JAPAN SOCIETY OF MECHANICAL ENGINEERS Series A
سال: 1997
ISSN: 0387-5008,1884-8338
DOI: 10.1299/kikaia.63.879