Fractography. .SIGMA. Phase Embrittlement of Duplex Stainless Steel Weldment.

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Kinetics of Sigma Phase Formation In a Duplex Stainless Steel

This work determines the kinetics of sigma phase formation in UNS S31803 Duplex Stainless Steel (DSS), describing the phase transformations that occur in isothermal aging between 700 and 900 °C for time periods up to 1032 hours, allowing the determination of the Time-Temperature-Precipitation (TTP) diagram for sigma phase and proposing a model to predict the kinetics of sigma phase formation us...

متن کامل

Study of creep cavitation in a stainless steel weldment

A study of creep cavities near reheat cracking in AISI Type 316H austenitic stainless steel headers, removed from long-time high temperature operation in nuclear power plants, is reported. It is shown how application of scanning electron microscopy (SEM), cryogenic fractography and small angle neutron scattering (SANS) can be applied, in a complementary way, to observe and quantify creep cavita...

متن کامل

Low-Temperature Mechanical Behavior of Super Duplex Stainless Steel with Sigma Precipitation

Experimental studies in various aspects have to be conducted to maintain stable applications of super duplex stainless steels (SDSS) because the occurrence rate of sigma phase, variable temperature and growth direction of sigma phase can influence mechanical performances of SDSS. Tensile tests of precipitated SDSS were performed under various temperatures to analyze mechanical and morphological...

متن کامل

Crystallography of Widmanstätten austenite in duplex stainless steel weld metal

Two kinds of austenite grow from d-ferrite during the cooling of the duplex stainless steel weld deposits studied here, Widmanstätten plates and allotriomorphs which precipitate at d–d grain boundaries. It is found using microtexture measurements that the preferred crystallographic orientation of the Widmanstätten austenite can be estimated using established theory if it is assumed that there i...

متن کامل

Local Approach to Fracture of an Aged Duplex Stainless Steel

The local approach to fracture (LAF) is a methodology aimed to calculate macroscopic fracture properties of a body, from the knowledge of the local stress strain field at the fracture site, and the modeling of the acting fracture mechanisms. In the present work, this method was applied to a CF8M steel, aged 30000 h at 325 °C, in order to elucidate if LAF could be able to describe the measured f...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Society of Materials Science, Japan

سال: 1997

ISSN: 1880-7488,0514-5163

DOI: 10.2472/jsms.46.592