Fractography and Tensile Properties of AA6061 Aluminium Alloy/Rice Husk Ash Silicon Nanocomposite

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Evaluation of Coal Waste Ash and Rice Husk Ash on Properties of Pervious Concrete Pavement

The use of pervious concrete has been significantly considered in recent years. This consideration is due to the properties of pervious concrete in relating to the environmental sustainability that is utilized in the effective management of the runoff from rainfall. Coal extraction and rice husk obtained from milling, produces wastes that have no application and followed by environmental pollut...

متن کامل

Effect of quartz-silicon dioxide particulate on tensile properties of aluminium alloy cast composites

This paper describes an experimental investigation of the tensile properties of quartz-silicon dioxide particulate reinforced LM6 aluminium alloy composite. In this experimental, quartzsilicon dioxide particulate reinforced LM6 composite were fabricated by carbon dioxide sand moulding process with variation of the particulate content on percentage of weight. Tensile tests were conducted to dete...

متن کامل

Wear behaviour of AA6061 aluminium alloy and its composites

This study investigates the wear resistance of four AA6061 MMCs together with the monolithic AA6061 alloy, all in the T6 condition, using a pin-on-disc test. In addition to the widely studied 20 vol.% Saffil MMCs, the present investigation considered a hybrid of 11% Saffil + 20% Sic, and a high volume fraction Sic, MMC. AA6061 + 60% Sic,. The wear behaviour against P400 Sic grit adhesive bonded...

متن کامل

Luminescence properties of silicon-cellulose nanocomposite

We have characterized the structure and luminescence properties for two-component material composed of nanocrystalline cellulose and nanocrystalline (less to 100 nm) silicon powder. An efficient and stable photoluminescence of nanocomposite, resistant to the influence of gas-phase oxidants, has been found. The obtained material has electret-like properties and demonstrates the possibility of mu...

متن کامل

Combine Use of Fly Ash and Rice Husk Ash in Concrete to Improve its Properties (RESEARCH NOTE)

This research paper describes the study of combined effect of Fly Ash (FA) and Rice Husk Ash (RHA) on properties of concrete as partial replacement of Ordinary Portland Cement (OPC). These by-products are having high pozzolanic reactivity. In this research, the composition of mix was used with 10% RHA along with 10, 20 and 30% FA as partial replacement of cement. In this study, the compressive ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: International Journal of Chemical Engineering

سال: 2020

ISSN: 1687-806X,1687-8078

DOI: 10.1155/2020/8818224