Fractography Analysis of Monolithic Epoxy with Tailored Topography

The topographical features of fractured tensile, flexural, K1C, and impact specimens of monolithic epoxy have been studied and correlated with mechanical properties and surface features of samples before fracture. The topographical features studied include waviness (Wa), roughness average (Ra), root mean square value (Rq), and maximum roughness height (Rmax or Rz). As surface notches generate t...

متن کامل

Fractography of Polymer Composites: Current Status and Future Issues

With the increasing prevalence of polymer composites in engineering applications, invariably mechanical failures of these components are occurring. Key to addressing this is fractographic analysis; the examination of fracture surfaces to deduce information about the damage and failure of components. The fractography of isotropic materials, particularly metals, has been used as a tool for many y...

متن کامل

Life Estimate of a Compressor Blade through Fractography

Failure analysis of fractured components provides some information about the causes and conditions of fracture. Fractography is an indispensable part of the failure analysis as it is usually the only means by which the failure mechanism can be established. By using fractography, some information such as component’s life, values of the stress intensity factor and the applied stress can be calcul...

متن کامل

Fatigue behaviour and fractography of extruded AZ80 magnesium alloys in very high cycle regime

In order to investigate the fatigue properties of extruded magnesium alloy in very high-cycle regime, rotary bending fatigue test was performed in ambient atmosphere at room temperature using the hourglass shaped specimens of AZ80 alloys extruded (Fspecimen) and treated by an artificial aging after extrusion (T5-specimen). From the experimental results, both specimens show a clear step-wise S-N...

متن کامل

Fractography of clinically fractured, implant-supported dental computer-aided design and computer-aided manufacturing crowns

Today, a substantial part of the dental crown production uses computer-aided design and computer-aided manufacturing (CAD/CAM) technology. A recent step in restorative dentistry is the replacement of natural tooth structure with pre-polymerized and machined resin-based methacrylic polymers. Recently, a new CAD/CAM composite was launched for the crown indication in the load-bearing area, but the...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Society of Materials Science, Japan

سال: 1974

ISSN: 1880-7488,0514-5163

DOI: 10.2472/jsms.23.479