Fractographic Evaluation of Medium Carbon Steels with Low Hot Ductility

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Determining the Hot Deformation Temperature Range of Medium Carbon Ni-Cr-Mo Low Alloy Steels using Hot Tensile and Hot Torsion Tests

The aim of this study was to investigate the suitable temperature range for hot deformation of three medium carbon Ni-Cr-Mo low alloy steels by hot tensile and hot torsion tests. Hot tensile tests were carried out in the te,prature range of 850-1150°C at a constant strain rate of 0.1 s-1 until fracture. Then, the tensile flow behavior, hot ductility and microstructural evolution of the steels w...

متن کامل

Analysis of Abrasive Wear Characterization and its Correlation with Structure for Low and Medium Carbon Steels

In most of the engineering applications, such as mining, metallurgy, agriculture; equipments are failed by the abrasive wear. The data as obtained form ministry of Research and Technology indicates that the percentage cost of abrasive wear in federal republic of German in metallurgy industry is 40%, mining industry 30%, agriculture 20% and production engineering 10%, and so the material selecti...

متن کامل

Prediction of Deformation Resistance of Low Carbon Steels during Hot Rolling

Phenomenological approach to the description of deformation resistance behaviour of steel and its microstructure development under the service hot rolling condition is still the most common useful and powerful. Utilising different experimental equipment such as torsion plastometer [1-5], compression plastometer [6-9], or advanced laboratory mills [10, 11] as well as different deformation techni...

متن کامل

Additively manufactured hierarchical stainless steels with high strength and ductility.

Many traditional approaches for strengthening steels typically come at the expense of useful ductility, a dilemma known as strength-ductility trade-off. New metallurgical processing might offer the possibility of overcoming this. Here we report that austenitic 316L stainless steels additively manufactured via a laser powder-bed-fusion technique exhibit a combination of yield strength and tensil...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Microscopy and Microanalysis

سال: 2002

ISSN: 1431-9276,1435-8115

DOI: 10.1017/s1431927602101280