Formation of Solidification and Eutectic Microstructures with Solidification Rates in the Single Crystal Superalloy CMSX 10

نویسندگان

چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Numerical Simulation and Optimization of Directional Solidification Process of Single Crystal Superalloy Casting

The rapid development of numerical modeling techniques has led to more accurate results in modeling metal solidification processes. In this study, the cellular automaton-finite difference (CA-FD) method was used to simulate the directional solidification (DS) process of single crystal (SX) superalloy blade samples. Experiments were carried out to validate the simulation results. Meanwhile, an i...

متن کامل

Effect of Solidification Behavior on Microstructures and Mechanical Properties of Ni-Cr-Fe Superalloy Investment Casting

The effect of solidification behavior on the microstructures and mechanical properties of Ni-Cr-Fe superalloy investment casting is given. Metallographic and image analysis have been used to quantitatively examine the microstructures' evolution. For the parts with the thickness of 3 mm and 24 mm, the volume fraction and maximum equivalent radius of the Laves phase increases from 0.3% to 1.2%, f...

متن کامل

Phase-Field Models for Eutectic Solidification

This article discusses two methods for modeling eutectic solidifi cation using the phase-field approach. First, a multi-phase-fi eld model is used to study the three-dimensional morphological evolution of binary eutectics. Performing the calculations in three dimensions allows observation of both lamellar and rod-like structures as well as transient phenomena such as lamellar fault motion, rod-...

متن کامل

Crystal Growth and Dendritic Solidification

We present a numerical method which computes the motion of complex solid/liquid boundaries in crystal growth. The model we solve includes physical effects such as crystalline anisotropy, surface tension, molecular kinetics and undercooling. The method is based on two ideas. First, the equations of motion are recast as a single history-dependent boundary integral equation on the solid/liquid bou...

متن کامل

Changes in Solidification Mode, and the Measurement of Cooling Rates following Solidification during Arc Welding

The solidification process in a weld pool has been shown to have a considerable influence upon the properties of the resultant weld. It influences the development of microstructure (Edvardsson et al., 1976), and determines the distribution of alloying elements, and hence the homogeneity of the weld. Previous work on the cooling behaviour of welds (Garland and Kirkwood, 1974; Svensson et al., 19...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Korean Journal of Materials Research

سال: 2008

ISSN: 1225-0562

DOI: 10.3740/mrsk.2008.18.11.577