Water-resistant Whey Protein Based Wood Adhesive Modified by Post-treated Phenol-formaldehyde Oligomers (pfo)
With the attempt to develop an environmentally safe whey protein-based adhesive with good water resistance, a low-molecular-weight PFO was used as a modifier, and the effects of scavengers on the formaldehyde emission and bond properties were investigated. Plywood evaluation and HPLC analysis indicated that the PFO synthesized with a low content of sodium hydroxide as a catalyst (NaOH/phenol mo...
متن کاملPerformance Characterization of Coatings on Treated-wood
Coating performance is greatly influenced by the properties of the wood substrate. This study was focused on evaluating the performance of coatings on both preservative- and thermally-treated wood. A number of commercially formulated semi-transparent stains Alkyd, Alkyd-Acrylic and PU were applied on four different types of preservative treated and heat-treated wood and their performances were ...
متن کاملExecutive Summary: Treated Wood
As part of the process outlined in Washington's Statewide Strategy to Recover Salmon: Extinction is Not an Option the Washington Departments of Fish and Wildlife, Ecology, and Transportation were charged to develop Aquatic Habitat Guidelines employing an integrated approach to marine, freshwater, and riparian habitat protection and restoration. Guidelines will be issued, as funding allows, in a...
متن کاملLiquefied Wood as a Partial Substitute of Melamine-urea- Formaldehyde and Urea-formaldehyde Resins
Maritime pine (Pinus pinaster) sawdust was used to produce liquefied wood by the polyhydric method with acid catalysis. The process was optimized to produce the highest amount of liquefied wood. Wood liquefied at 160oC for 90 min was used in the adhesion tests. The bond strength of veneer glued with ureaformaldehyde and melamine-urea-formaldehyde resins and several mixtures of liquefied wood wi...
متن کاملSynthesis and Cure Kinetics of Liquefied Wood/Phenol/ Formaldehyde Resins
Wood liquefaction was conducted at a 2/1 phenol/wood ratio in two different reactors: (1) an atmospheric three-necked flask reactor and (2) a sealed Parr reactor. The liquefied wood mixture (liquefied wood, unreacted phenol, and wood residue) was further condensed with formaldehyde under acidic conditions to synthesize two novolac-type liquefied wood/phenol/formaldehyde (LWPF) resins: LWPF1 (th...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Wood Preservation
سال: 1994
ISSN: 0287-9255,1884-0116
DOI: 10.5990/jwpa.20.2