The stress concentration of In718 superalloy after friction welding and compare with Mar-M247 and In718 welded joints
Friction stir welding (FSW) is a new method that the joining is carried out by friction between two metals and heat creation. The stress concentration phenomena in welded joint cause the stress increasing in welded zone. In this research, modeling and analysis of similar junction of IN718 and Mar-M247 and non-similar junction of IN718-Mar-M247 superalloys were performed by ANSYS Software and fi...
متن کاملThe stress concentration of In718 superalloy after friction welding and compare with Mar-M247 and In718 welded joints
Friction stir welding (FSW) is a new method that the joining is carried out by friction between two metals and heat creation. The stress concentration phenomena in welded joint cause the stress increasing in welded zone. In this research, modeling and analysis of similar junction of IN718 and Mar-M247 and non-similar junction of IN718-Mar-M247 superalloys were performed by ANSYS Software and fi...
متن کاملeffect of bataine and sulphate supplement on wool and milk characteristics and lambs performance in naine ewes
تعداد 20 رأس میش نژاد نائینی 6+-24 ماهه، با میانگین وزن 2/3-+40 کیلوگرم، همراه با 20 رأس بره های آنها در قالب طرح کاملا تصادفی اثر بتائین و مکمل سولفات بر خصوصیات شیر و پشم و عملکرد بره ها بررسی شد. میش ها بطور تصادفی در چهار تیمار قرار گرفتند. تیمارها عبارت بودند از: 1-گروه شاهد 2-بتائین (05/0 درصد ماده خشک) 3-سولفات (24/0 سولفور درصد ماده خشک 4-بتائین هرماه با سولفات. جیره غذائی طبق nrc با مح...
15 صفحه اولlearning style, self efficacy and intrinsic motivation as predictors of iranian ielts reading comprehension
this thesis attempts to measure learning styles, self efficacy and intrinsic motivation as predictors of iranian ielts reading comprehension. in order to address this issue, a quantitative study was conducted on some randomly selected intact students at ferdowsi university. these two groups were assigned as they were undergraduate (ba=91) and graduate (ma =74) students; they were all aged betwe...
Compressive Strength and Workability Characteristics of Low-Calcium Fly ash-based Self-Compacting Geopolymer Concrete
Due to growing environmental concerns of the cement industry, alternative cement technologies have become an area of increasing interest. It is now believed that new binders are indispensable for enhanced environmental and durability performance. Self-compacting Geopolymer concrete is an innovative method and improved way of concreting operation that does not require vibration for placing it an...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Materials Science and Engineering: A
سال: 2015
ISSN: 0921-5093
DOI: 10.1016/j.msea.2015.06.093