Flotation studies of copper ore Majdanpek to enhance copper recovery and concentrate grade with different collectors

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Optimization of parameters affecting recovery of copper from Sarcheshmeh low-grade sulfide ore using Bioleaching

In this work, the parameters affecting the recovery of copper from the low-grade sulfide minerals of Sarcheshmeh Copper Mine were studied. A low-grade sulfide ore was used with a copper grade of 0.25%, which was about 28% of the mineral oxide, and the sulfide minerals made up the rest. Much more sulfide minerals were found to be pyrite and most of the gangue minerals were quartz, anorthite, bio...

متن کامل

Investigation of Flotation Parameters for Copper Recovery from Enargite and Chalcopyrite Mixed Ore

A flotation pre-treatment study for the separation of enargite (Cu3AsS4) from chalcopyrite (CuFeS2) ores of different origins was investigated in this work. The copper ore bearing enargite mineral contained 5.87mass% As and 16.50mass% Cu while the chalcopyrite bearing ore contained 0.32mass% As and 21.63mass% Cu. The two ore samples were mixed at 7 : 3 (enargite : chalcopyrite) by weight ratio ...

متن کامل

Recovery of Copper from Copper Slag and Copper Slag Flotation Tailings by Oxidative Leaching

Copper smelter slag and copper smelter slag flotation tailings were leached using sulphuric acid solutions, without or with the addition of either ferric sulphate or hydrogen peroxide. Copper extraction from the slag was typically found to be twice as high as that from the slag flotation tailings. Hydrogen peroxide was determined to be the best lixiviant. Thus, copper and iron extractions were ...

متن کامل

Modofication of the Sarcheshmeh copper complex flotation circuit in response to a reduction in feed grade

The new copper processing plant of the Sarcheshmeh copper complex consists of two parallel circuits. After a primary crushing, the ore is sent to a SAG mill, and the product is further ground in a ball mill. The overflow of the hydrocyclones is fed to a flotation circuit that contains 8 rougher tank cells (RCS130), 3 cleaner cells (RCS50), 5 scavenger cells (RCS50), and a flotation column (as r...

متن کامل

Vitrification of copper flotation waste.

The vitrification of an hazardous iron-rich waste (W), arising from slag flotation of copper production, was studied. Two glasses, containing 30wt% W were melted for 30min at 1400 degrees C. The first batch, labeled WSZ, was obtained by mixing W, blast furnace slag (S) and zeolite tuff (Z), whereas the second, labeled WG, was prepared by mixing W, glass cullet (G), sand and limestone. The glass...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Mining and Metallurgy A: Mining

سال: 2019

ISSN: 1450-5959,2560-3159

DOI: 10.5937/jmma1901053s