Flexural strength and fracture toughness of two different lithium disilicate ceramics

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Flexural strength and microstructure of two lithium disilicate glass ceramics for CAD/CAM restoration in the dental clinic

OBJECTIVES There has been a growing interest in glass ceramic systems with good esthetics, high fracture resistance and bonding durability, and simplified fabrication techniques using CAD/CAM. The aim of this study is to compare flexural strength before and after heat treatment of two lithium disilicate CAD/CAM blocks, IPS e.max CAD (Ivoclar Vivadent) and Rosetta SM (Hass), and to observe their...

متن کامل

Correction: Effect of Heat-Pressing Temperature and Holding Time on the Microstructure and Flexural Strength of Lithium Disilicate Glass-Ceramics

There are errors in affiliation 1 for authors Fu Wang, Zhiguo Chai, Jung Gao, Hui Wang, and Jihua Chen and affiliation 2 for author Zaixi Deng. Affiliation 1 should be: State Key Laboratory of Military Stomatology, Department of Prosthodontics, School of Stomatology, Fourth Military Medical University, Xi’an, PR China Affiliation 2 should be: State Key Laboratory of Military Stomatology, Depart...

متن کامل

Effect of Heat-Pressing Temperature and Holding Time on the Microstructure and Flexural Strength of Lithium Disilicate Glass-Ceramics

The present study aimed to evaluate the influence of various heat-pressing procedures (different holding time and heat pressing temperature) on the microstructure and flexural strength of lithium disilicate glass ceramic. An experimental lithium silicate glass ceramic (ELDC) was prepared from the SiO2-Li2O-K2O-Al2O3-ZrO2-P2O5 system and heat-pressed following different procedures by varying tem...

متن کامل

Effects of Different Polishing Protocols on Lithium Disilicate Ceramics.

The aim of this study was to evaluate the effect of different polishing protocols on surface roughness and morphology of lithium disilicate ceramics (IPS e.max CAD). Fifty ceramic bars (2.0x3.0x2.5 mm) were produced and randomly divided into five groups (n=10), according to surface treatments: C: Control; Cer: Ceramaster (60 s); CW: cloth wheel with large-grit diamond (30 s) + cloth wheel with ...

متن کامل

A Comparison of Tensile Bond Strength between Low Translucency and High Translucency Lithium Disilicate Ceramics Using Two Different Resin Cements

Objectives: To compare two different dual-curing resins cement interfaces between low translucency and high translucency lithium disilicate glass-ceramics in vitro. M~aterials and Methods: ISO 11405 was modeled by using a standardized dumb-bell test to compare the tensile bond strength of two different resin cement interfaces ofa low translucency lithium disilicate ceramic to a high translucenc...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Dental Materials Journal

سال: 2020

ISSN: 0287-4547,1881-1361

DOI: 10.4012/dmj.2019-045