Ferritic steel that ASTM E1921 master curve failed to characterize its fracture toughness temperature dependence

نویسندگان

چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Inhomogeneity Screening Criterion for the Astm E1921 T0 Estimate Based on the Sintap Lower-tail Methodology

The Master Curve brittle fracture toughness estimation method described in the ASTM E1921-11 test standard is based on a theoretical scatter and size effect assumption and makes use of a maximum likelihood estimation method to determine the fracture toughness transition temperature T0. The estimation method in E1921-11 is valid only for macroscopically homogeneous steels. If the steel is inhomo...

متن کامل

Constraint-Based Master Curve Analysis of a Nuclear Reactor Pressure Vessel Steel results from an experimental programme carried out within the IAEA CRP-8 project

This report presents the outcome of four fracture test series, addressing the ductile-to-brittle toughness behaviour of a nuclear reactor pressure vessel steel. Each test series corresponds to a specific test specimen geometry, tensile or three-point-bend, with a given degree of crack-tip constraint. A brief overview is given of available constraint-based fracture mechanics methodologies in the...

متن کامل

Strong Ferritic – Steel Welds

There are many steels which are stronger than 2000 MPa, with toughness values exceeding 100 MPa m and which have been in commercial service for many decades. Examples include the marageing alloys and carbide–free bainitic steels. By contrast, welding consumables with a proof strength in excess of 1000 MPa are few and far between. This is because whereas wrought steels can be thermomechanically ...

متن کامل

Influence of Texture on Impact Toughness of Ferritic Fe-20Cr-5Al Oxide Dispersion Strengthened Steel

Fe-based oxide dispersion strengthened (ODS) steels are oriented to applications where high operating temperatures and good corrosion resistance is paramount. However, their use is compromised by their fracture toughness, which is lower than other competing ferritic-martenstic steels. In addition, the route required in manufacturing these alloys generates texture in the material, which induces ...

متن کامل

Theory for Hydrogen Desorption in Ferritic Steel

After a concise review of the analytical models available for the interpretation of thermal desorption rates for hydrogen effusion from steel, a numerical method that incorporates the essence of local equilibrium and detrapping kinetics has been implemented to account for the real complexity of practical experiments. For example, the model permits the treatment of multiple kinds of traps, uses ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Transactions of the JSME (in Japanese)

سال: 2019

ISSN: 2187-9761

DOI: 10.1299/transjsme.18-00431