Fermi level unpinning of GaSb (100) using plasma enhanced atomic layer deposition of Al2O3

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Atomic layer deposition of Al2O3 on GaSb using in situ hydrogen plasma exposure

In this report, we study the effectiveness of hydrogen plasma surface treatments for improving the electrical properties of GaSb/Al2O3 interfaces. Prior to atomic layer deposition of an Al2O3 dielectric, p-GaSb surfaces were exposed to hydrogen plasmas in situ, with varying plasma powers, exposure times, and substrate temperatures. Good electrical interfaces, as indicated by capacitance-voltage...

متن کامل

Introduction to (plasma-enhanced) atomic layer deposition

Film growth by the atomic layer deposition (ALD) method relies on alternate pulsing of the precursor gases and vapors into a vacuum chamber and their subsequent chemisorption on the substrate surface (Fig. 1) [1,2]. The different steps in the process are saturative such that ALD film growth is self-limiting yielding one submonolayer of film per deposition cycle. ALD has some unique characterist...

متن کامل

Direct Growth of Al2O3 on Black Phosphorus by Plasma-Enhanced Atomic Layer Deposition

Growing high-quality and uniform dielectric on black phosphorus is challenging since it is easy to react with O2 or H2O in ambient. In this work, we have directly grown Al2O3 on BP using plasma-enhanced atomic layer deposition (PEALD). The surface roughness of BP with covered Al2O3 film can reduce significantly, which is due to the removal of oxidized bubble in BP surface by oxygen plasma. It w...

متن کامل

High-k GaAs metal insulator semiconductor capacitors passivated by ex-situ plasma- enhanced atomic layer deposited AlN for Fermi-level unpinning

Please cite the original version: Jussila, H. & Mattila, P. & Oksanen, J. & Perros, A. & Riikonen, J. & Bosund, M. & Varpula, A. & Huhtio, T. & Lipsanen, Harri & Sopanen, M. 2012. High-k GaAs metal insulator semiconductor capacitors passivated by ex-situ plasma-enhanced atomic layer deposited AlN for Fermi-level unpinning. Applied Physics Letters. Volume 100, Issue 7. P. 071606/1-4. ISSN 0003-6...

متن کامل

The Role of Magnetic Field in Atomic Layer Deposition of Al2O3 Thin Films Enhanced by Radio Frequency Plasma

As a media aluminum oxide (Al2O3) thin films deposited by radio frequency plasma-assisted atomic layer deposition (RF-PA-ALD) method were employed to explore the magnetic field effect. Different from normal plasma-assisted ALD (PA-ALD) technology a magnetic field was applied during the whole deposition process. With this novel ALD technology it obtains that the deposition rate in each cycle of ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Applied Physics Letters

سال: 2010

ISSN: 0003-6951,1077-3118

DOI: 10.1063/1.3492847