Fatigue crack initiation in a notched single-crystal superalloy component

In this paper, the fatigue crack initiation in notched single-crystal test specimens of material MD2 is investigated and analysed. A critical plane approach is adopted, in which the total strain ranges on the discrete slip planes are evaluated. Furthermore, a Coffin-Manson type of expression is used to describe the number of cycles to fatigue crack initiation. This relation is determined from a...

متن کامل

Creep Crack Growth Simulation of Ni-base Superalloy

The purpose of this study is to develop a numerical approach to simulate the creep cracking of a Ni-base superalloy. The approach is based in continuum damage mechanics (CDM) and uses the classic Kachanov-Rabotnov constitutive equations for creep deformation and damage evolution. Creep damage takes the form of defects such as microcracks, cavities, voids, etc. A numerical crack growth algorithm...

متن کامل

Effect of thermal treatment on the fatigue crack propagation behavior of a new Ni-base superalloy

Effect of thermal treatment on the fatigue crack propagation behavior of a new Ni-base superalloy Xingbo Liu a,*, ling Xu a, Ever Barbero a, Wei-Di Cao b, Richard L. Kennedy b a West Virginia University, Morgantown, WV 26506-6106, USA b Allvac, an AT! Technologies Company, Monroe, NC 28111-5030, USA Received 22 October 2006; received in revised form 23 March 2007; accepted 10 May 2007 The effec...

متن کامل

Fretting on the cubic face of a single-crystal Ni-base superalloy at room temperature

Fretting experiments were conducted on the (10 0) crystal (cubic) face of a single crystal Ni-base superalloy in two directions, /10 0S and /110S, to study the effect of crystallographic orientation on the fretting response in both partial slip and gross slip regimes. The study involved point contacts using a tungsten carbide (WC) ball with radius 10 mm tested at room temperature. Ball indentat...

متن کامل

Thermomechanical Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy

A continuum crystal plasticity model is used to simulate the material behavior of a directionally solidified Ni-base superalloy, DS GTD-111, in the longitudinal and transverse orientations. Isothermal uniaxial fatigue tests with hold times and creep tests are conducted at temperatures ranging from room temperature (RT) to 1038°C to characterize the deformation response. The constitutive model i...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: TRANSACTIONS OF THE JAPAN SOCIETY OF MECHANICAL ENGINEERS Series A

سال: 1996

ISSN: 0387-5008,1884-8338

DOI: 10.1299/kikaia.62.1146