Fatigue behaviour of the superalloy IN 713C under LCF-, HCF- and superimposed LCF/HCF-loading
نویسندگان
چکیده
منابع مشابه
Modelling combined HCF-LCF fatigue crack growth under the influence of LCF overload
Fatigue crack growth (FCG) rates have previously been reported in forged Ti6Al-4V aero-engine disk material under the conjoint action of LCF and HCF cycles at room temperature. It is found that systematic increases in LCF overload, applied prior to the commencement of the HCF cycles, reduce the contribution of the HCF cycles to crack growth rates. The application of overload also enhances the s...
متن کاملBehaviour of Corroded Stud Shear Connectors under Fatigue Loading
Experimental investigation was conducted on corroded composite push-out specimens to study the behavior of shear studs subjected to fatigue loading. A total of eight standard EC4 push-out specimens were tested. The expected corrosion rate of test specimens ranged from 0 to 50%. The main purpose of these tests was to determine the fatigue life and the reduction effect caused by the corrosion on ...
متن کاملthe analysis of the role of the speech acts theory in translating and dubbing hollywood films
از محوری ترین اثراتی که یک فیلم سینمایی ایجاد می کند دیالوگ هایی است که هنرپیش گان فیلم میگویند. به زعم یک فیلم ساز, یک شیوه متأثر نمودن مخاطب از اثر منظوره نیروی گفتارهای گوینده, مثل نیروی عاطفی, ترس آور, غم انگیز, هیجان انگیز و غیره, است. این مطالعه به بررسی این مسأله مبادرت کرده است که آیا نیروی فراگفتاری هنرپیش گان به مثابه ی اعمال گفتاری در پنج فیلم هالیوودی در نسخه های دوبله شده باز تولید...
15 صفحه اولInvestigation of the Heat Treatment Effect on Microstructures and Phases of Inconel 713C Superalloy
The application of Inconel 713C is very vast in different industries such as in automobiles, aircrafts, boilers and turbines. In this paper, Inconel 713C specimens were solutionized at 1000 and 1200 °C for 1 hours in order to study changes in phases and the structure of alloy to modify the γ' phase. The optical and the scanning electron microscopy were used to investigate the structure and the ...
متن کاملthe survey of the virtual higher education in iran and the ways of its development and improvement
این پژوهش با هدف "بررسی وضعیت موجود آموزش عالی مجازی در ایران و راههای توسعه و ارتقای آن " و با روش توصیفی-تحلیلی و پیمایشی صورت پذیرفته است. بررسی اسنادو مدارک موجود در زمینه آموزش مجازی نشان داد تعداد دانشجویان و مقاطع تحصیلی و رشته محل های دوره های الکترونیکی چندان مطلوب نبوده و از نظر کیفی نیز وضعیت شاخص خدمات آموزشی اساتید و وضعیت شبکه اینترنت در محیط آموزش مجازی نامطلوب است.
ذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Procedia Engineering
سال: 2010
ISSN: 1877-7058
DOI: 10.1016/j.proeng.2010.03.146